| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 电能存储系统用锂蓄电池和电池组 安全要求 | 1 | 电压测量公差 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.3 a) Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | ||
| 2 | 2 | 电流测量公差 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.3 b) Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 3 | 3 | 温度测量公差 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.3 c) Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 4 | 4 | 时间测量公差 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.3 d) Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 5 | 5 | 尺寸测量公差 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.3 e) Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 6 | 6 | 质量测量公差 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.3 f) Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 7 | 7 | 电池样品实际容量 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.6.3 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 8 | 8 | 引入导线测试或连接总电阻 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.6.1 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 9 | 9 | 高温外部短路 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 6.1 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 10 | 10 | 静电放电预处理 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 4.6.4 b) Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB/T 17626.2《电磁兼容 试验和测量技术 静电放电抗扰度试验》 | |||
| 11 | 11 | 标识和警示说明耐久性 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 5.3.3 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 12 | 12 | 耐高温永久性标识 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 5.3.3 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 13 | 13 | 过充电 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 6.2 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 14 | 14 | 强制放电 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 6.3 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 15 | 15 | 低气压 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.1 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB/T 2423.21《电工电子产品环境试验 第2部分:试验方法 试验M:低气压》 | |||
| 16 | 16 | 温度循环 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.2 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB/T 2423.22《环境试验 第2部分:试验方法 试验N:温度变化》 | |||
| 17 | 17 | 振动 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.3 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB/T 2423.10《环境试验 第2部分:试验方法 试验Fc:振动(正弦)》 | |||
| 18 | 18 | 加速度冲击 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.4 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB/T 2423.5《环境试验 第2部分:试验方法 试验Ea和导则:冲击》 | |||
| 19 | 19 | 重物冲击 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.5 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 20 | 20 | 挤压 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.6 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 21 | 21 | 浅刺 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.7 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 22 | 22 | 热滥用 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.8 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 23 | 23 | 跌落 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 7.9 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 24 | 24 | 过压充电控制 | 040905 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 8.3 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 25 | 25 | 过流充电控制 | 040905 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 8.4 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 26 | 26 | 欠压放电控制 | 040905 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 8.5 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 27 | 27 | 过热控制 | 040905 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 8.6 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 28 | 28 | 耐异常热 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 9.1 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB/T 5169.21《电工电子产品着火危险试验 第21部分:非正常热 球压试验方法》 | |||
| 29 | 29 | 阻燃性 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 9.2 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB/T 5169.16;GB 31241—2022 附录G | |||
| 30 | 30 | 运输和安装过程中的电气绝缘检查 | 040901 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 9.3 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB 4943.1—2022《音视频、信息技术和通信技术设备 第1部分:安全要求》 | |||
| 31 | 31 | 运输和安装过程中的短路保护 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 9.4 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 32 | 32 | 反向连接保护 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 9.5 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 33 | 33 | 电池组系统抗电强度 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 9.6 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements 引用方法:GB 4943.1—2022 5.4.8、5.4.9 | |||
| 34 | 34 | 电池热失控 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 9.7.1 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||
| 35 | 35 | 电池组系统热扩散 | 040999 | 《电能存储系统用锂蓄电池和电池组 安全要求》GB44240-2024 9.7.2 Secondary lithium cells and batteries used in electrical energy storage systems—Safety requirements | |||