项目
限值 / 检出限 / 定量限
单位
出处
标称电压
扣式锂-二氧化锰电池= 3.0 V (CR927)
= 3.0 V (CR1025)
= 3.0 V (CR1216)
= 3.0 V (CR1220)
= 3.0 V (CR1225)
= 3.0 V (CR1616)
= 3.0 V (CR1620)
= 3.0 V (CR1632)
= 3.0 V (CR2012)
= 3.0 V (CR2016)
= 3.0 V (CR2025)
= 3.0 V (CR2320)
= 3.0 V (CR2032)
= 3.0 V (CR2330)
= 3.0 V (CR2335)
= 3.0 V (CR2430)
= 3.0 V (CR2354)
= 3.0 V (CR3032)
= 3.0 V (CR2450)
= 3.0 V (CR2477)
= 3.0 V (CR11108)V6.2.2 表6
最大开路电压
扣式锂-二氧化锰电池≤ 3.7 V (CR927)
≤ 3.7 V (CR1025)
≤ 3.7 V (CR1216)
≤ 3.7 V (CR1220)
≤ 3.7 V (CR1225)
≤ 3.7 V (CR1616)
≤ 3.7 V (CR1620)
≤ 3.7 V (CR1632)
≤ 3.7 V (CR2012)
≤ 3.7 V (CR2016)
≤ 3.7 V (CR2025)
≤ 3.7 V (CR2320)
≤ 3.7 V (CR2032)
≤ 3.7 V (CR2330)
≤ 3.7 V (CR2335)
≤ 3.7 V (CR2430)
≤ 3.7 V (CR2354)
≤ 3.7 V (CR3032)
≤ 3.7 V (CR2450)
≤ 3.7 V (CR2477)
≤ 3.7 V (CR11108)V6.2.2 表6
最大外形尺寸-直径
扣式锂-二氧化锰电池≤ 9.5 mm (CR927)
≤ 10.0 mm (CR1025)
≤ 12.5 mm (CR1216)
≤ 12.5 mm (CR1220)
≤ 12.5 mm (CR1225)
≤ 16.0 mm (CR1616)
≤ 16.0 mm (CR1620)
≤ 16.0 mm (CR1632)
≤ 20.0 mm (CR2012)
≤ 20.0 mm (CR2016)
≤ 20.0 mm (CR2025)
≤ 23.0 mm (CR2320)
≤ 20.0 mm (CR2032)
≤ 23.0 mm (CR2330)
≤ 23.0 mm (CR2335)
≤ 24.5 mm (CR2430)
≤ 23.0 mm (CR2354)
≤ 30.0 mm (CR3032)
≤ 24.5 mm (CR2450)
≤ 24.5 mm (CR2477)
≤ 11.6 mm (CR11108)mm6.2.2 表6
最大外形尺寸-高度
扣式锂-二氧化锰电池≤ 2.7 mm (CR927)
≤ 2.5 mm (CR1025)
≤ 1.6 mm (CR1216)
≤ 2.0 mm (CR1220)
≤ 2.5 mm (CR1225)
≤ 1.6 mm (CR1616)
≤ 2.0 mm (CR1620)
≤ 3.2 mm (CR1632)
≤ 1.2 mm (CR2012)
≤ 1.6 mm (CR2016)
≤ 2.5 mm (CR2025)
≤ 2.0 mm (CR2320)
≤ 3.2 mm (CR2032)
≤ 3.0 mm (CR2330)
≤ 3.5 mm (CR2335)
≤ 3.0 mm (CR2430)
≤ 5.4 mm (CR2354)
≤ 3.2 mm (CR3032)
≤ 5.0 mm (CR2450)
≤ 7.7 mm (CR2477)
≤ 10.8 mm (CR11108)mm6.2.2 表6
放电条件-电阻
扣式锂-二氧化锰电池= 62 kΩ (CR927)
= 68 kΩ (CR1025)
= 62 kΩ (CR1216)
= 62 kΩ (CR1220)
= 30 kΩ (CR1225)
= 30 kΩ (CR1616)
= 47 kΩ (CR1620)
= 15 kΩ (CR1632)
= 30 kΩ (CR2012)
= 30 kΩ (CR2016)
= 15 kΩ (CR2025)
= 15 kΩ (CR2320)
= 15 kΩ (CR2032)
= 15 kΩ (CR2330)
= 15 kΩ (CR2335)
= 15 kΩ (CR2430)
= 7.5 kΩ (CR2354)
= 7.5 kΩ (CR3032)
= 7.5 kΩ (CR2450)
= 4.7 kΩ (CR2477)
= 15 kΩ (CR11108)kΩ6.2.2 表6
放电条件-每天放电时间
扣式锂-二氧化锰电池= 24 h (CR927)
= 24 h (CR1025)
= 24 h (CR1216)
= 24 h (CR1220)
= 24 h (CR1225)
= 24 h (CR1616)
= 24 h (CR1620)
= 24 h (CR1632)
= 24 h (CR2012)
= 24 h (CR2016)
= 24 h (CR2025)
= 24 h (CR2320)
= 24 h (CR2032)
= 24 h (CR2330)
= 24 h (CR2335)
= 24 h (CR2430)
= 24 h (CR2354)
= 24 h (CR3032)
= 24 h (CR2450)
= 24 h (CR2477)
= 24 h (CR11108)h6.2.2 表6
放电条件-终止电压
扣式锂-二氧化锰电池= 2.0 V (CR927)
= 2.0 V (CR1025)
= 2.0 V (CR1216)
= 2.0 V (CR1220)
= 2.0 V (CR1225)
= 2.0 V (CR1616)
= 2.0 V (CR1620)
= 2.0 V (CR1632)
= 2.0 V (CR2012)
= 2.0 V (CR2016)
= 2.0 V (CR2025)
= 2.0 V (CR2320)
= 2.0 V (CR2032)
= 2.0 V (CR2330)
= 2.0 V (CR2335)
= 2.0 V (CR2430)
= 2.0 V (CR2354)
= 2.0 V (CR3032)
= 2.0 V (CR2450)
= 2.0 V (CR2477)
= 2.0 V (CR11108)V6.2.2 表6
最小平均放电量(初始期)
扣式锂-二氧化锰电池≥ 480 h (CR927)
≥ 630 h (CR1025)
≥ 480 h (CR1216)
≥ 700 h (CR1220)
≥ 480 h (CR1225)
≥ 480 h (CR1616)
≥ 900 h (CR1620)
≥ 550 h (CR1632)
≥ 530 h (CR2012)
≥ 675 h (CR2016)
≥ 540 h (CR2025)
≥ 590 h (CR2320)
≥ 920 h (CR2032)
≥ 1320 h (CR2330)
≥ 1350 h (CR2335)
≥ 1300 h (CR2430)
≥ 1260 h (CR2354)
≥ 1250 h (CR3032)
≥ 1200 h (CR2450)
≥ 1300 h (CR2477)
≥ 620 h (CR11108)h6.2.2 表6
标称电压
异形锂-二氧化锰电池= 6.0 V (CR-P2(2CP4036))
= 6.0 V (2CR5(2CP3845))V6.2.3 表7
最大开路电压
异形锂-二氧化锰电池≤ 7.4 V (CR-P2(2CP4036))
≤ 7.4 V (2CR5(2CP3845))V6.2.3 表7
外形尺寸
GB 8897.2—2005 · 异形锂-二氧化锰电池= (CR-P2(2CP4036):参见GB 8897.2—2005)
= (2CR5(2CP3845):参见GB 8897.2—2005)mm6.2.3 表7
放电条件-电阻/电流
异形锂-二氧化锰电池= 200 Ω (CR-P2(2CP4036) 200 Ω)
= 900 mA (CR-P2(2CP4036) 900 mA)
= 200 Ω (2CR5(2CP3845) 200 Ω)
= 900 mA (2CR5(2CP3845) 900 mA)Ω/mA6.2.3 表7
放电条件-每天放电时间
异形锂-二氧化锰电池= 24 h (CR-P2(2CP4036) 200 Ω条件)
= (CR-P2(2CP4036) 900 mA条件:放电3 s,停放27 s,每天24 h)
= 24 h (2CR5(2CP3845) 200 Ω条件)
= (2CR5(2CP3845) 900 mA条件:放电3 s,停放27 s,每天24 h)h6.2.3 表7
标称电压
圆柱形锂-亚硫酰氯电池 ER14250= 3.6 V (ER14250)V6.3.1 表8
最大开路电压
圆柱形锂-亚硫酰氯电池 ER14250≤ 3.9 V (ER14250)V6.3.1 表8
最大外形尺寸-直径
圆柱形锂-亚硫酰氯电池 ER14250≤ 14.5 mm (ER14250)mm6.3.1 表8
最大外形尺寸-高度
圆柱形锂-亚硫酰氯电池 ER14250≤ 25.0 mm (ER14250)mm6.3.1 表8
最小平均放电量(初始期)
圆柱形锂-亚硫酰氯电池 ER14250≥ 450 h (ER14250, 放电条件 2.0 mA/1.6 kΩ, 每天放电24 h, 终止电压2.0 V)h6.3.1 表8
标称电压
矩形锂-亚硫酰氯电池 2EP3863= 7.2 V (2EP3863)V6.3.2 表9
最大开路电压
矩形锂-亚硫酰氯电池 2EP3863≤ 7.8 V (2EP3863)V6.3.2 表9
尺寸
GB 8897.2—2005 · 矩形锂-亚硫酰氯电池 2EP3863= (2EP3863, 参见GB 8897.2—2005)mm6.3.2 表9
最小平均放电量(初始期)
矩形锂-亚硫酰氯电池 2EP3863≥ 650 h (2EP3863, 放电条件 3.3 kΩ, 每天放电24 h, 终止电压3.0 V)h6.3.2 表9
标称电压
圆柱形锂-二氧化硫电池 WR14505= 2.9 V (WR14505)V6.4.1 表10