| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 硅单晶切割片和研磨片 | 1 | 直径允许偏差 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | ||
| 2 | 2 | 厚度(中心点) | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 3 | 3 | 厚度允许偏差 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 4 | 4 | 总厚度变化 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 5 | 5 | 弯曲度 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 6 | 6 | 翘曲度 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 7 | 7 | 主参考面长度 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 8 | 8 | 副参考面长度 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 9 | 9 | 切口深度 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers 引用方法:GB/T 26067《硅片切口尺寸测试方法》 | |||
| 10 | 10 | 切口角度 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers 引用方法:GB/T 26067《硅片切口尺寸测试方法》 | |||
| 11 | 11 | 主参考面直径 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.3 表1 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 12 | 12 | 表面取向偏离度(正晶向) | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.4.2 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 13 | 13 | 表面取向偏离度(偏晶向) | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.4.2 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 14 | 14 | 主参考面取向 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.5.1 表2、5.5.2 表3 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 15 | 15 | 副参考面位置 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.5.1 表2 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 16 | 16 | 切口基准轴取向 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.5.2 表3 Monocrystalline silicon as cut wafers and lapped wafers | |||
| 17 | 17 | 崩边 | 025299 | 《硅单晶切割片和研磨片》GB/T12965-2018 5.7.1 表4 Monocrystalline silicon as cut wafers and lapped wafers 引用方法:GB/T 6624《硅抛光片表面质量目测检验方法》 | |||