| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 额定电压 10 kV 架空绝缘电缆 | 1 | 导体最少单线根数 | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | ||
| 2 | 2 | 导体直径(参考值) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 3 | 3 | 导体屏蔽层最小厚度(近似值) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 4 | 4 | 绝缘标称厚度(薄绝缘) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 5 | 5 | 绝缘标称厚度(普通绝缘) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 6 | 6 | 绝缘屏蔽层标称厚度 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 7 | 7 | 20°C时导体电阻(硬铜芯) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 8 | 8 | 20°C时导体电阻(软铜芯) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 9 | 9 | 20°C时导体电阻(铝芯) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 10 | 10 | 20°C时导体电阻(铝合金芯) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 11 | 11 | 导体拉断力(硬铜芯) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 12 | 12 | 导体拉断力(铝芯) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 13 | 13 | 导体拉断力(铝合金芯) | 040503 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表3 Aerial insulated cables for rated voltage of 10 kV | |||
| 14 | 14 | 钢承载绞线拉断力 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表4 Aerial insulated cables for rated voltage of 10 kV | |||
| 15 | 15 | 铝合金承载绞线拉断力 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.1 表4 Aerial insulated cables for rated voltage of 10 kV | |||
| 16 | 16 | 绝缘电阻 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.7.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 17 | 17 | 交流电压试验电压 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.7.3 表5 Aerial insulated cables for rated voltage of 10 kV | |||
| 18 | 18 | 局部放电量 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 19 | 19 | 负载下伸长率 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.8.4 表7 Aerial insulated cables for rated voltage of 10 kV | |||
| 20 | 20 | 冷却后永久伸长率 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.8.4 表7 Aerial insulated cables for rated voltage of 10 kV | |||
| 21 | 21 | tanδ(室温) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.5 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 3048.11—2007《》 | |||
| 22 | 22 | 冲击电压试验(普通绝缘结构电缆) | 040501 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.8.1 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 3048.8—2007《》 | |||
| 23 | 23 | 冲击电压试验(轻型薄绝缘结构电缆) | 040501 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.8.1 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 3048.8—2007《》 | |||
| 24 | 24 | 泄漏电流 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.10 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 3048.7—2007《》 | |||
| 25 | 25 | 抗张强度(老化前) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.12.1 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 2951.1和.2—1997 | |||
| 26 | 26 | 断裂伸长率(老化前) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.12.1 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 2951.1和.2—1997 | |||
| 27 | 27 | 抗张强度变化率(空气老化后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.12.1 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 2951.1和.2—1997 | |||
| 28 | 28 | 断裂伸长率变化率(空气老化后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.12.1 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 2951.1和.2—1997 | |||
| 29 | 29 | 断裂伸长率(空气老化后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.12.1 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 2951.1和.2—1997 | |||
| 30 | 30 | 熔体指数(老化前) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.12.2 Aerial insulated cables for rated voltage of 10 kV 引用方法:GB/T 3682—2000《》 | |||
| 31 | 31 | 绝缘粘附力(滑脱力) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.13 Aerial insulated cables for rated voltage of 10 kV | |||
| 32 | 32 | 抗张强度变化率(耐候试验) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.15 Aerial insulated cables for rated voltage of 10 kV | |||
| 33 | 33 | 伸长率变化率(耐候试验) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.15 Aerial insulated cables for rated voltage of 10 kV | |||
| 34 | 34 | 抗张强度变化率(耐候试验对比) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.15 Aerial insulated cables for rated voltage of 10 kV | |||
| 35 | 35 | 伸长率变化率(耐候试验对比) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.15 Aerial insulated cables for rated voltage of 10 kV | |||
| 36 | 36 | 外半导电层剥离力 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 7.9.16 Aerial insulated cables for rated voltage of 10 kV | |||
| 37 | 37 | 密度 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号1 Aerial insulated cables for rated voltage of 10 kV | |||
| 38 | 38 | 抗张强度(老化前) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号2 Aerial insulated cables for rated voltage of 10 kV | |||
| 39 | 39 | 断裂伸长(老化前) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号2 Aerial insulated cables for rated voltage of 10 kV | |||
| 40 | 40 | 空气老化温度 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号3 Aerial insulated cables for rated voltage of 10 kV | |||
| 41 | 41 | 空气老化持续时间 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号3 Aerial insulated cables for rated voltage of 10 kV | |||
| 42 | 42 | 抗张强度变化率(空气老化后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号3.1 Aerial insulated cables for rated voltage of 10 kV | |||
| 43 | 43 | 断裂伸长变化率(空气老化后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号3.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 44 | 44 | 断裂伸长(空气老化后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号3.3 Aerial insulated cables for rated voltage of 10 kV | |||
| 45 | 45 | 维卡软化点 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号4 Aerial insulated cables for rated voltage of 10 kV | |||
| 46 | 46 | 冲击脆化温度 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号5、表A.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 47 | 47 | 耐环境应力开裂 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号6 Aerial insulated cables for rated voltage of 10 kV | |||
| 48 | 48 | 熔体指数 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号7 Aerial insulated cables for rated voltage of 10 kV | |||
| 49 | 49 | 介电常数 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号8 Aerial insulated cables for rated voltage of 10 kV | |||
| 50 | 50 | 介质损耗角正切(20°C) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号9 Aerial insulated cables for rated voltage of 10 kV | |||
| 51 | 51 | 介电强度 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号10 Aerial insulated cables for rated voltage of 10 kV | |||
| 52 | 52 | 负荷下伸长率(热延伸200°C,15min) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号12 Aerial insulated cables for rated voltage of 10 kV | |||
| 53 | 53 | 冷却后永久变形(热延伸200°C,15min) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号13 Aerial insulated cables for rated voltage of 10 kV | |||
| 54 | 54 | 凝胶含量 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号14 Aerial insulated cables for rated voltage of 10 kV | |||
| 55 | 55 | 抗张强度变化率(光老化42d后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号15 Aerial insulated cables for rated voltage of 10 kV | |||
| 56 | 56 | 断裂伸长率变化率(光老化42d后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.1 序号15 Aerial insulated cables for rated voltage of 10 kV | |||
| 57 | 57 | 抗拉强度 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 58 | 58 | 断裂伸长率 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 59 | 59 | 断裂伸长率(空气箱老化后) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 60 | 60 | 负荷伸长率(热延伸200°C/0.2MPa/15min) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 61 | 61 | 冷却后永久变形(热延伸200°C/0.2MPa/15min) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 62 | 62 | 剥离力 | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 63 | 63 | 体积电阻率(23°C) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.2 Aerial insulated cables for rated voltage of 10 kV | |||
| 64 | 64 | 体积电阻率(90°C) | 040599 | 《额定电压 10 kV 架空绝缘电缆》GB/T14049-2008 表A.2 Aerial insulated cables for rated voltage of 10 kV | |||