| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 单、双面挠性印制板分规范 | 1 | 导线缺口或针孔 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.1 表1 Sectional specification for single and double sided flexible printed board | ||
| 2 | 2 | 连接盘缺损面积 | 040606 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.1 b) Sectional specification for single and double sided flexible printed board | |||
| 3 | 3 | 孔周焊盘缺损 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.1 c) Sectional specification for single and double sided flexible printed board | |||
| 4 | 4 | 导线间的残留铜或突出部分 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.2 表2 Sectional specification for single and double sided flexible printed board | |||
| 5 | 5 | 宽阔区域内残留铜或突出距印制板外缘距离 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.3 Sectional specification for single and double sided flexible printed board | |||
| 6 | 6 | 宽阔区域内残留铜或突出与相邻导体图形距离 | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.3 Sectional specification for single and double sided flexible printed board | |||
| 7 | 7 | 导线表面凹坑深度 | 040615 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.4 表3 Sectional specification for single and double sided flexible printed board | |||
| 8 | 8 | 导体分层 | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.5 表4 Sectional specification for single and double sided flexible printed board | |||
| 9 | 9 | 导体上的划痕深度 | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.2.7 表5 Sectional specification for single and double sided flexible printed board | |||
| 10 | 10 | 导线变色 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.2.3 表6 Sectional specification for single and double sided flexible printed board | |||
| 11 | 11 | 导线外的气泡 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.1 表7 Sectional specification for single and double sided flexible printed board | |||
| 12 | 12 | 导线上的气泡 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.1 表7 Sectional specification for single and double sided flexible printed board | |||
| 13 | 13 | 总气泡 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.1 表7 Sectional specification for single and double sided flexible printed board | |||
| 14 | 14 | 覆盖层未层压 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.1 表7 Sectional specification for single and double sided flexible printed board | |||
| 15 | 15 | 非导电性夹杂物厚度t | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.2 表8 Sectional specification for single and double sided flexible printed board | |||
| 16 | 16 | 非导电性夹杂物宽度W | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.2 表8 Sectional specification for single and double sided flexible printed board | |||
| 17 | 17 | 非导电性夹杂物长度l | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.2 表8 Sectional specification for single and double sided flexible printed board | |||
| 18 | 18 | 分层及剥离 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.3 Sectional specification for single and double sided flexible printed board | |||
| 19 | 19 | 覆盖层粘接剂的溢出及覆盖涂层的渗出尺寸l | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.4 表9 Sectional specification for single and double sided flexible printed board | |||
| 20 | 20 | 感光性阻焊剂的渗出尺寸l | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.4 表9 Sectional specification for single and double sided flexible printed board | |||
| 21 | 21 | 连接盘最小可焊环宽W | 040606 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.4 表10 Sectional specification for single and double sided flexible printed board | |||
| 22 | 22 | 覆盖涂层及感光性阻焊跳印(飞白)处导体焊料附着 | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.3.5 Sectional specification for single and double sided flexible printed board | |||
| 23 | 23 | 镀金层缺损面积比例 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 表11 Sectional specification for single and double sided flexible printed board | |||
| 24 | 24 | 镀金层缺损(接触部位) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 表11 Sectional specification for single and double sided flexible printed board | |||
| 25 | 25 | 镀金层缺损(直接接触部位) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 表11 Sectional specification for single and double sided flexible printed board | |||
| 26 | 26 | 镀金层缺陷宽度W1 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 表12 Sectional specification for single and double sided flexible printed board | |||
| 27 | 27 | 镀金层缺陷长度L | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 表12 Sectional specification for single and double sided flexible printed board | |||
| 28 | 28 | 可焊性镀涂层缺损宽度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 c) Sectional specification for single and double sided flexible printed board | |||
| 29 | 29 | 可焊性镀涂层缺损长度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 c) Sectional specification for single and double sided flexible printed board | |||
| 30 | 30 | 连接盘镀金层缺陷面积比例 | 040606 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 c) Sectional specification for single and double sided flexible printed board | |||
| 31 | 31 | 孔边缘镀层缺损 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.1 c) Sectional specification for single and double sided flexible printed board | |||
| 32 | 32 | 镀覆孔内空洞数 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.2 Sectional specification for single and double sided flexible printed board | |||
| 33 | 33 | 镀覆孔镀层空洞面积总和S总 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.2 表13 Sectional specification for single and double sided flexible printed board | |||
| 34 | 34 | 导线与覆盖层之间镀层渗出或焊料芯吸m1、m2 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.3 表14 Sectional specification for single and double sided flexible printed board | |||
| 35 | 35 | 导线与基底膜之间镀层渗出或焊料芯吸 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.3 表15 Sectional specification for single and double sided flexible printed board | |||
| 36 | 36 | 镀金层外观 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.4 表16 Sectional specification for single and double sided flexible printed board | |||
| 37 | 37 | 可焊性镀层表面发黑 | 040615 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.4.4 b) Sectional specification for single and double sided flexible printed board | |||
| 38 | 38 | 撕裂或缺口 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.5.1 Sectional specification for single and double sided flexible printed board | |||
| 39 | 39 | 毛刺高度n | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.5.2 Sectional specification for single and double sided flexible printed board | |||
| 40 | 40 | 丝状毛刺长度l1 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.5.3 Sectional specification for single and double sided flexible printed board | |||
| 41 | 41 | 丝状毛刺垂度l2 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.5.3 Sectional specification for single and double sided flexible printed board | |||
| 42 | 42 | 与增强材料之间的夹杂物引起的突出(p) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.1 a) Sectional specification for single and double sided flexible printed board | |||
| 43 | 43 | 夹杂物大小占粘接面积比例 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.1 b) Sectional specification for single and double sided flexible printed board | |||
| 44 | 44 | 与元件孔或外形边缘相连接的夹杂物 | 040606 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.1 c) Sectional specification for single and double sided flexible printed board | |||
| 45 | 45 | 外形边缘伸出的丝状非导电性夹杂物长度(l) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.1 d) Sectional specification for single and double sided flexible printed board | |||
| 46 | 46 | 增强材料与印制板间气泡面积占比(热固粘接剂) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.2 Sectional specification for single and double sided flexible printed board | |||
| 47 | 47 | 增强材料与印制板间气泡面积占比(其他类型粘接剂) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.2 Sectional specification for single and double sided flexible printed board | |||
| 48 | 48 | 印制插头端部气泡和翘起 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.2 Sectional specification for single and double sided flexible printed board | |||
| 49 | 49 | 增强材料裂缝 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.3 a) 表17 Sectional specification for single and double sided flexible printed board | |||
| 50 | 50 | 增强材料缺损长度(l) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.6.3 b) Sectional specification for single and double sided flexible printed board | |||
| 51 | 51 | 表面热固型粘接剂 | 040615 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.1 a) 表18 Sectional specification for single and double sided flexible printed board | |||
| 52 | 52 | 表面残留的助焊剂 | 040615 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.1 b) 表19 Sectional specification for single and double sided flexible printed board | |||
| 53 | 53 | 残留的金属颗粒 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.1 c) 表20 Sectional specification for single and double sided flexible printed board | |||
| 54 | 54 | 残留的粘接剂 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.1 d) 表21 Sectional specification for single and double sided flexible printed board | |||
| 55 | 55 | 皱褶 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.2 Sectional specification for single and double sided flexible printed board | |||
| 56 | 56 | 压痕深度(g) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.3 表22 Sectional specification for single and double sided flexible printed board | |||
| 57 | 57 | 基底膜压痕深度(g) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.4 a) 表23 Sectional specification for single and double sided flexible printed board | |||
| 58 | 58 | 基底膜划痕深度(i)与基底膜厚度(t)之比 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.4 b) 表24 Sectional specification for single and double sided flexible printed board | |||
| 59 | 59 | 覆盖层及覆盖涂层压痕深度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.5 a) 表25 Sectional specification for single and double sided flexible printed board | |||
| 60 | 60 | 覆盖层及覆盖涂层划痕深度(i)与厚度(t)之比 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.5 b) 表26 Sectional specification for single and double sided flexible printed board | |||
| 61 | 61 | 标记符号 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.5.7.6 Sectional specification for single and double sided flexible printed board | |||
| 62 | 62 | 外形尺寸公差(≤100 mm) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.2 表27 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 63 | 63 | 厚度公差 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.3 表28 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 64 | 64 | 成品孔径公差(t≥0.8 mm) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.4.2 表29 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 65 | 65 | 成品孔径公差(0.2<t<0.8 mm) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.4.2 表29 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 66 | 66 | 成品孔径公差(t≤0.2 mm) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.4.2 表29 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 67 | 67 | 镀覆孔最小孔径及公差 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.4.3 表30 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 68 | 68 | 导体宽度公差(0.05≤W<0.10 mm) | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.5 表31 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 69 | 69 | 导体宽度公差(0.10≤W<0.20 mm) | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.5 表31 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 70 | 70 | 导体宽度公差(0.20≤W<0.30 mm) | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.5 表31 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 71 | 71 | 导体宽度公差(0.30≤W<0.50 mm) | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.5 表31 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 72 | 72 | 导体宽度公差(W≥0.50 mm) | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.5 表31 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 73 | 73 | 导体节距累积公差 | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.6 表32 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 第6章 | |||
| 74 | 74 | 孔中心距 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.7、5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 75 | 75 | 导线到板边缘最小距离 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.8 Sectional specification for single and double sided flexible printed board | |||
| 76 | 76 | 孔位公差 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.9.1 Sectional specification for single and double sided flexible printed board | |||
| 77 | 77 | 连接盘的最小可焊环宽 | 040606 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.9.3 Sectional specification for single and double sided flexible printed board | |||
| 78 | 78 | 焊垫的有效面积 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.9.3 Sectional specification for single and double sided flexible printed board | |||
| 79 | 79 | 允许的外形偏移j | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.9.4 Sectional specification for single and double sided flexible printed board | |||
| 80 | 80 | 冲切外形的偏移 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.9.5 Sectional specification for single and double sided flexible printed board | |||
| 81 | 81 | 压敏胶或热固粘接剂的偏移V(包括粘接剂的溢出) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.10 Sectional specification for single and double sided flexible printed board | |||
| 82 | 82 | 镀覆孔的镀铜层最小厚度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.6.11、5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 83 | 83 | 导线剥离强度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.7.1.2 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 中7.2 | |||
| 84 | 84 | 覆盖层剥离强度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.7.1.2 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 中7.2 | |||
| 85 | 85 | 增强材料剥离强度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.7.1.2 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 中7.2 | |||
| 86 | 86 | 拉脱强度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.7.2.2、5.6.3.1 表44 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 中7.2.1、7.2.2 | |||
| 87 | 87 | 镀层附着力 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.7.3.2、5.6.2.3 表42 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 中8.1.1 | |||
| 88 | 88 | 可焊性 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.7.4.2、5.6.2.3 表42 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 中8.2 | |||
| 89 | 89 | 耐挠曲性 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.7.5.2、表44 序号5 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 中7.3 | |||
| 90 | 90 | 耐折性 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.7.6.2、表44 序号6 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 中7.4 | |||
| 91 | 91 | 化学性能 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.8.2 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 中8.1.3 | |||
| 92 | 92 | 表面绝缘电阻(验收态) | 040601 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.9.2.2、表44 序号3 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 中6.1.1 方法3a | |||
| 93 | 93 | 表面绝缘电阻(湿热处理后) | 040601 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.9.2.2、表44 序号8 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 湿热试验方法 | |||
| 94 | 94 | 表面耐电压 | 040615 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.9.2.3、表44 序号4 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 中6.5.1 | |||
| 95 | 95 | 开路 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.9.2.4 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 中6.2.2 | |||
| 96 | 96 | 短路 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.9.2.4 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 中6.2.1 | |||
| 97 | 97 | 镀覆孔的耐热冲击(镀通孔电阻变化率) | 040601 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.10.2.4 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 中9.2(热应力) | |||
| 98 | 98 | 耐离子迁移 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.10.2.5 Sectional specification for single and double sided flexible printed board | |||
| 99 | 99 | 清洁度(离子污染度) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.11.2 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 4677—2002 第10章 | |||
| 100 | 100 | 阻燃性 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 4.12.2、表44 序号11 Sectional specification for single and double sided flexible printed board 引用方法:GB/T 13557—2017 中10.2 | |||
| 101 | 101 | 导线外观 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 102 | 102 | 覆盖层及覆盖涂层外观 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 103 | 103 | 镀层外观 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 104 | 104 | 外形边缘和冲切孔的外观 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 105 | 105 | 增强材料的外观 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 106 | 106 | 其他 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 107 | 107 | 外形尺寸 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 108 | 108 | 厚度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 109 | 109 | 孔 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 110 | 110 | 导线宽度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 111 | 111 | 导体节距的累积公差 | 040609 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 112 | 112 | 导线到板边缘的最小距离 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 113 | 113 | 位置公差 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 114 | 114 | 板与增强材料压敏胶或热固粘接剂的偏移 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 115 | 115 | 耐热冲击性(高温浸渍) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 116 | 116 | 镀覆孔的耐热冲击 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.2.3 表42 Sectional specification for single and double sided flexible printed board | |||
| 117 | 117 | 剥离强度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 5.6.3.1 表44 Sectional specification for single and double sided flexible printed board | |||
| 118 | 118 | 耐化学性 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号7 Sectional specification for single and double sided flexible printed board | |||
| 119 | 119 | 耐湿性 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号9 Sectional specification for single and double sided flexible printed board | |||
| 120 | 120 | 耐热冲击(高低温循环) | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号10 Sectional specification for single and double sided flexible printed board | |||
| 121 | 121 | 导线电阻 | 040601 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号12 Sectional specification for single and double sided flexible printed board | |||
| 122 | 122 | 温度循环 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号13;附录A Sectional specification for single and double sided flexible printed board | |||
| 123 | 123 | 耐离子迁移性 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号14;附录B Sectional specification for single and double sided flexible printed board | |||
| 124 | 124 | 晶须 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号15;附录C Sectional specification for single and double sided flexible printed board | |||
| 125 | 125 | 盐雾测试 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号16 Sectional specification for single and double sided flexible printed board | |||
| 126 | 126 | 清洁度 | 040699 | 《单、双面挠性印制板分规范》GB/T14515-2019 表44 序号17 Sectional specification for single and double sided flexible printed board | |||