| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 厚膜集成电路用氧化铝陶瓷基片 | 1 | 裂纹 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | ||
| 2 | 2 | 瓷疤 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 3 | 3 | 凸脊 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 4 | 4 | 毛刺 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 5 | 5 | 划痕 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 6 | 6 | 缺损 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 7 | 7 | 凹坑 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 8 | 8 | 斑点(锈斑) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 9 | 9 | 斑点(色斑) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 10 | 10 | 斑点(暗斑) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.1 表1 Alumina ceramic substrates for thick film integrated circuits | |||
| 11 | 11 | 长度、宽度(L) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.1 表2 Alumina ceramic substrates for thick film integrated circuits | |||
| 12 | 12 | 厚度 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.1 表2 Alumina ceramic substrates for thick film integrated circuits | |||
| 13 | 13 | 翘曲度 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.1 表2 Alumina ceramic substrates for thick film integrated circuits | |||
| 14 | 14 | 垂直度(基片) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.1 表2 Alumina ceramic substrates for thick film integrated circuits | |||
| 15 | 15 | 平行度(基片) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.1 表2 Alumina ceramic substrates for thick film integrated circuits | |||
| 16 | 16 | 孔径及偏差 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.2.1 表3 Alumina ceramic substrates for thick film integrated circuits | |||
| 17 | 17 | 孔的位置及偏差 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.2.2 Alumina ceramic substrates for thick film integrated circuits | |||
| 18 | 18 | 划线边缘与第一条划线间的尺寸 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.3 表4 Alumina ceramic substrates for thick film integrated circuits | |||
| 19 | 19 | 划线线条间的位置 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.3 表4 Alumina ceramic substrates for thick film integrated circuits | |||
| 20 | 20 | 基片掰开后两对应分切片间的偏差 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.3 表4 Alumina ceramic substrates for thick film integrated circuits | |||
| 21 | 21 | 垂直度(分切片) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.3 表4 Alumina ceramic substrates for thick film integrated circuits | |||
| 22 | 22 | 平行度(分切片) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.2.3 表4 Alumina ceramic substrates for thick film integrated circuits | |||
| 23 | 23 | 实际氧化铝含量 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 4.3 Alumina ceramic substrates for thick film integrated circuits | |||
| 24 | 24 | 基片氧化铝含量(质量分数) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 25 | 25 | 表面粗糙度(Ra) | 040615 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 26 | 26 | 体积密度 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 27 | 27 | 透液性 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 28 | 28 | 抗折强度 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 29 | 29 | 硬度(维氏) | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 30 | 30 | 线膨胀系数 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 31 | 31 | 导热率 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 32 | 32 | 抗热震性 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 33 | 33 | 体积电阻率 | 040601 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 34 | 34 | 击穿强度 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 35 | 35 | 介电常数 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||
| 36 | 36 | 损耗正切值 | 040699 | 《厚膜集成电路用氧化铝陶瓷基片》GB/T14619-2013 5.3 表5 Alumina ceramic substrates for thick film integrated circuits | |||