| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 | 1 | SF6气体设计压力(20℃,相对压力) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 4.3 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | ||
| 2 | 2 | 最低功能压力(相对压力) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 4.3 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 3 | 3 | 终端轴线与垂直线夹角 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 4.4 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories 引用方法:GB/T4109—2008《交流电压高于1000V 的绝缘套管》 | |||
| 4 | 4 | 压接型导体连接管铜含量 | 040503 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 6.1 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories 引用方法:GB/T1527—2006《铜及铜合金拉制管》 | |||
| 5 | 5 | 真空漏增试验压力漏增值(B-A) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 8.4.1.2 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 6 | 6 | 真空漏增试验残压A | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 8.4.1.2 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 7 | 7 | 真空计分辨率 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 8.4.1.2 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 8 | 8 | 户外终端淋雨工频电压 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 8.4.3 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories 引用方法:GB/T16927.1 | |||
| 9 | 9 | 抗张强度 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表A.1 序号1 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 10 | 10 | 断裂伸长率 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表A.1 序号1 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 11 | 11 | 抗张强度变化率 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表A.1 序号2 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 12 | 12 | 伸长率的变化率 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表A.1 序号2 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 13 | 13 | 体积电阻率(23 ℃) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表A.1 序号3、表B.1 序号1 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 14 | 14 | tanδ | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表B.1 序号1 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 15 | 15 | 介电常数 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表B.1 序号1 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 16 | 16 | 短时工频击穿电场强度 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表B.1 序号1 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 17 | 17 | 热变形温度 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表B.1 序号2 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 18 | 18 | 外观 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表C.1 序号1、表C.2 序号1 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 19 | 19 | 运动黏度(25 ℃) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表C.1 序号2 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 20 | 20 | 闪点 | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表C.1 序号3、表C.2 序号2 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 21 | 21 | 折光指数(25 ℃) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表C.1 序号4、表C.2 序号3 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 22 | 22 | 击穿电压(电极间距2.5mm) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表C.1 序号5、表C.2 序号4 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 23 | 23 | 体积电阻率(25 ℃) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表C.1 序号6、表C.2 序号5 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||
| 24 | 24 | 挥发度(条件:150 ℃,3h) | 040599 | 《额定电压220kV(Um=252kV)交联聚乙烯绝缘电力电缆及其附件 第3部分:电缆附件》GB/T18890.3-2015 表C.1 序号7 Power cables with cross-linked polyethylene insulation and their accessories for rated voltage of 220kV (Um=252kV)—Part 3: Accessories | |||