项目
限值 / 检出限 / 定量限
单位
出处
着火电压 Uf
附录A · 氙灯= 400 V (XMZ3-60L)
= 360 V (XMZ4-50L)
= 500 V (XMZ4-100L)
= 400 V (XMZ5-75L)
= 480 V (XMZ5-100L)
= 400 V (XMZ6-90L)
= 450 V (XMZ6-100L)
= 680 V (XMZ6-125L)
= 650 V (XMZ6-150L)
= 550 V (XMZ7-130L)
= 600 V (XMZ7-150L)
= 550 V (XMZ8-120P)V4.3 表3
标准触发电压幅值
附录A · 氙灯≥ 15 kV (所有型号)kV4.3 表3
标准触发电压脉宽
附录A · 氙灯≥ 1.6 μs (所有型号)μs4.3 表3
电阻系数 K0
附录A · 氙灯= 25.6 Ω·A^{1/2} (XMZ3-60L)
= 16.0 Ω·A^{1/2} (XMZ4-50L)
= 32.0 Ω·A^{1/2} (XMZ4-100L)
= 19.2 Ω·A^{1/2} (XMZ5-75L)
= 25.6 Ω·A^{1/2} (XMZ5-100L)
= 19.2 Ω·A^{1/2} (XMZ6-90L)
= 21.3 Ω·A^{1/2} (XMZ6-100L)
= 26.7 Ω·A^{1/2} (XMZ6-125L)
= 32.0 Ω·A^{1/2} (XMZ6-150L)
= 23.8 Ω·A^{1/2} (XMZ7-130L)
= 27.4 Ω·A^{1/2} (XMZ7-150L)
= 19.2 Ω·A^{1/2} (XMZ8-120P)
= 32.4 Ω·A^{1/2} (XMZ15-380L)
= 37.6 Ω·A^{1/2} (XMZ17-500L)
= 95.6 Ω·A^{1/2} (XMZ17-1 270L)
= 59.0 Ω·A^{1/2} (XMZ31-1 430L)
= 56.4 Ω·A^{1/2} (XMZ42-1 850L)Ω·A^{1/2}4.3 表3
爆炸能量常数 Kex
附录A · 氙灯≥ 21.6 W·μs^{1/2} (XMZ3-60L)
≥ 24.0 W·μs^{1/2} (XMZ4-50L)
≥ 48.0 W·μs^{1/2} (XMZ4-100L)
≥ 45.0 W·μs^{1/2} (XMZ5-75L)
≥ 60.0 W·μs^{1/2} (XMZ5-100L)
≥ 64.8 W·μs^{1/2} (XMZ6-90L)
≥ 72.0 W·μs^{1/2} (XMZ6-100L)
≥ 90.0 W·μs^{1/2} (XMZ6-125L)
≥ 108 W·μs^{1/2} (XMZ6-150L)
≥ 109 W·μs^{1/2} (XMZ7-130L)
≥ 126 W·μs^{1/2} (XMZ7-150L)
≥ 115 W·μs^{1/2} (XMZ8-120P)
≥ 684 W·μs^{1/2} (XMZ15-380L)
≥ 1020 W·μs^{1/2} (XMZ17-500L)
≥ 2590 W·μs^{1/2} (XMZ17-1 270L)
≥ 3520 W·μs^{1/2} (XMZ31-1 430L)
≥ 9320 W·μs^{1/2} (XMZ42-1 850L)W·μs^{1/2}4.3 表3
最大平均功率(自然冷却)
附录A · 氙灯= 90 W (XMZ3-60L)
= 101 W (XMZ4-50L)
= 201 W (XMZ4-100L)
= 188 W (XMZ5-75L)
= 251 W (XMZ5-100L)
= 271 W (XMZ6-90L)
= 302 W (XMZ6-100L)
= 377 W (XMZ6-125L)
= 452 W (XMZ6-150L)
= 457 W (XMZ7-130L)
= 528 W (XMZ7-150L)
= 483 W (XMZ8-120P)W4.3 表3
最大平均功率(强迫空冷)
附录A · 氙灯= 181 W (XMZ3-60L)
= 201 W (XMZ4-50L)
= 402 W (XMZ4-100L)
= 377 W (XMZ5-75L)
= 503 W (XMZ5-100L)
= 543 W (XMZ6-90L)
= 603 W (XMZ6-100L)
= 754 W (XMZ6-125L)
= 905 W (XMZ6-150L)
= 915 W (XMZ7-130L)
= 1060 W (XMZ7-150L)
= 965 W (XMZ8-120P)W4.3 表3
最大平均功率(液体冷却)
附录A · 氙灯= 1700 W (XMZ3-60L)
= 1890 W (XMZ4-50L)
= 3770 W (XMZ4-100L)
= 3530 W (XMZ5-75L)
= 4710 W (XMZ5-100L)
= 5090 W (XMZ6-90L)
= 5660 W (XMZ6-100L)
= 7070 W (XMZ6-125L)
= 8480 W (XMZ6-150L)
= 8580 W (XMZ7-130L)
= 9900 W (XMZ7-150L)
= 9050 W (XMZ8-120P)W4.3 表3
灯头耐压
附录A · 氙灯= 50 kV (XMZ15-380L)
= 50 kV (XMZ17-500L)
= 50 kV (XMZ17-1 270L)
= 55 kV (XMZ31-1 430L)
= 60 kV (XMZ42-1 850L)kV4.3 表3
灯头漏电流
附录A · 氙灯≤ 1 μA (每只灯头在额定耐压下)μA4.3 表3 注b
额定寿命
6.5 · 氙灯≥ 1000000 次 (fx=0.2时)次5.9
个别寿命
6.5 · 氙灯≥ 500000 次 (个别寿命不低于额定寿命的50%)次5.9