| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 室内装饰装修用水性木器涂料 | 1 | 在容器中状态 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | |||
| 2 | 2 | 细度 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 1724 | ||||
| 3 | 3 | 不挥发物 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 1725 | ||||
| 4 | 4 | 干燥时间-表干 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 1728—1979 表干中乙法 | ||||
| 5 | 5 | 干燥时间-实干 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 1728—1979 实干中甲法 | ||||
| 6 | 6 | 贮存稳定性[(50±2)°C,7d] | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 7 | 7 | 耐冻融性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 9755—2001 中5.5 | ||||
| 8 | 8 | 涂膜外观 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 9 | 9 | 光泽(60°) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 9754 | ||||
| 10 | 10 | 打磨性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 11 | 11 | 硬度(擦伤) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 6739 | ||||
| 12 | 12 | 附着力(划格间距2mm) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 9286—1998《》 | ||||
| 13 | 13 | 耐冲击性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1、6.4.12 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 14 | 14 | 抗粘连性[500g,(50±2)°C/4h] | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 15 | 15 | 耐磨性(750g/500r) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 1768 | ||||
| 16 | 16 | 耐划伤性(100g) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 9279 | ||||
| 17 | 17 | 耐水性(24h) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 18 | 18 | 耐沸水性(15min) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 19 | 19 | 耐碱性(50g/LNaHCO3,1h) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 20 | 20 | 耐醇性(50%,1h) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 21 | 21 | 耐污染性(1h)-醋 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 22 | 22 | 耐污染性(1h)-绿茶 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 23 | 23 | 耐干热性[(70±2)°C,15min] | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 4893.3—2005《》 | ||||
| 24 | 24 | 耐黄变性(168h)ΔE* | 《室内装饰装修用水性木器涂料》GB/T23999-2009 表1 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 25 | 25 | 抗粘连性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.13 Water based coatings for woodenware for indoor decorating and refurbishing | ||||
| 26 | 26 | 耐磨性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.14 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 1768 | ||||
| 27 | 27 | 耐划伤性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.15 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 9279 | ||||
| 28 | 28 | 耐水性(常温) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.16 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 4893.1—2005《》 | ||||
| 29 | 29 | 耐沸水性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.16 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 4893.1—2005《》 | ||||
| 30 | 30 | 耐碱性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.17 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 4893.1—2005《》 | ||||
| 31 | 31 | 耐醇性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.18 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 4893.1—2005《》 | ||||
| 32 | 32 | 耐污染性(耐醋) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.19 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 4893.1—2005《》 | ||||
| 33 | 33 | 耐污染性(耐茶) | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.19 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 4893.1—2005《》 | ||||
| 34 | 34 | 耐干热性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.20 Water based coatings for woodenware for indoor decorating and refurbishing 引用方法:GB/T 4893.3—2005《》 | ||||
| 35 | 35 | 耐黄变性 | 《室内装饰装修用水性木器涂料》GB/T23999-2009 6.4.21 Water based coatings for woodenware for indoor decorating and refurbishing | ||||