| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆 | 1 | GFRP圆杆杨氏模量 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 7.4.7 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | ||
| 2 | 2 | KFRP圆杆杨氏模量 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 7.4.7 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | |||
| 3 | 3 | 芳纶丝束杨氏模量 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 7.4.7 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | |||
| 4 | 4 | 挤包内衬层厚度 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 7.6.3 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | |||
| 5 | 5 | 绕包内衬层厚度 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 7.6.4 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | |||
| 6 | 6 | 挤包护套标称厚度 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 7.8.3 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | |||
| 7 | 7 | 标志计米长度误差 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 8.4 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | |||
| 8 | 8 | 最大衰减系数(1310 nm) | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 10.2.4.2 表8 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | |||
| 9 | 9 | 最大衰减系数(1550 nm) | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 10.2.4.2 表8 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) | |||
| 10 | 10 | 长期压扁力 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 10.4.5.3.1 表9 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) 引用方法:GB/T 7424.2—2008 试验方法-E3 | |||
| 11 | 11 | 短暂压扁力 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 10.4.5.3.1 表9 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) 引用方法:GB/T 7424.2—2008 试验方法-E3 | |||
| 12 | 12 | 光纤附加衰减(长期压扁) | 040508 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 10.4.5.3.1 表9 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) 引用方法:GB/T 7424.2—2008 试验方法-E3 | |||
| 13 | 13 | 光纤附加衰减(短暂压扁) | 040508 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 10.4.5.3.1 表9 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) 引用方法:GB/T 7424.2—2008 试验方法-E3 | |||
| 14 | 14 | 单模光纤允许光纤附加衰减 | 040508 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 10.4.6.2.1 表10 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) 引用方法:GB/T 7424.2—2008 试验方法-F1 | |||
| 15 | 15 | 滴流试验温度 | 040599 | 《额定电压 1 kV(Um=1.2 kV)及以下光纤复合低压电缆》GB/T29839-2013 10.4.6.4.1 表11 Optical fiber composite low-voltage cable for rated voltages up to and including 1 kV(Um=1.2 kV) 引用方法:GB/T 7424.2—2008 试验方法-F6 | |||