| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 电子装联高质量内部互连用焊锡膏 | 1 | 焊锡粉化学成分 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.1 Requirements for solder paste for high-quality interconnections in electronics assembly | |||
| 2 | 2 | 焊锡粉杂质含量 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.2 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 3 | 3 | 最大颗粒尺寸 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.3 表1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 4 | 4 | 少于1%质量分数颗粒尺寸 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.3 表1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 5 | 5 | 至少80%质量分数颗粒尺寸 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.3 表1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 6 | 6 | 至少90%质量分数颗粒尺寸 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.3 表1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 7 | 7 | 最多10%质量分数颗粒尺寸 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.3 表1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 8 | 8 | 焊锡粉形状(球形粉和近球形粉质量之和) | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.4 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 9 | 9 | 合金粉末含量质量分数 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.5 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 10 | 10 | 黏度 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.6、7.3.2、7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 11 | 11 | 塌陷(0.20mm模板,0.63mm×2.03mm图形,方法6.5.2.2a) | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.7.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 12 | 12 | 塌陷(0.20mm模板,0.33mm×2.03mm图形,方法6.5.2.2a) | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.7.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 13 | 13 | 塌陷(0.10mm模板,0.33mm×2.03mm图形,方法6.5.2.2a) | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.7.2 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 14 | 14 | 塌陷(0.10mm模板,0.20mm×2.03mm图形,方法6.5.2.2a) | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.7.2 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 15 | 15 | 锡珠试验评级 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.8 表2 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 16 | 16 | 粘附性(粘附力最小值) | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.9 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 17 | 17 | 润湿性评级 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.10 表3 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 18 | 18 | 助焊剂性能和类型 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 5.11 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 19 | 19 | 合金粉末含量 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.3.2、7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 20 | 20 | 塌陷 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.3.2、7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 21 | 21 | 润湿性 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.3.2、7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 22 | 22 | 合金成分 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 23 | 23 | 杂质含量 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 24 | 24 | 尺寸分布 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 25 | 25 | 形状 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 26 | 26 | 锡珠试验 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 27 | 27 | 卤素含量 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 28 | 28 | 干燥度 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 29 | 29 | 铜板腐蚀 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 30 | 30 | 铜镜腐蚀 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 31 | 31 | 绝缘电阻 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||
| 32 | 32 | 电迁移 | 《电子装联高质量内部互连用焊锡膏》GB/T31475-2015 7.4.1 Requirements for solder paste for high-quality interconnections in electronics assembly | ||||