| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 玻镁平板 | 1 | 表观密度 | 100101 | 《玻镁平板》GB/T33544-2017 4.1 表1 Glass fiber and magnesium cement board | ||
| 2 | 2 | 长度 | 100199 | 《玻镁平板》GB/T33544-2017 4.2 表2 Glass fiber and magnesium cement board | |||
| 3 | 3 | 宽度 | 100199 | 《玻镁平板》GB/T33544-2017 4.2 表2 Glass fiber and magnesium cement board | |||
| 4 | 4 | 厚度 | 100199 | 《玻镁平板》GB/T33544-2017 4.2 表2 Glass fiber and magnesium cement board | |||
| 5 | 5 | 长度尺寸允许偏差 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.2 表3 Glass fiber and magnesium cement board | |||
| 6 | 6 | 宽度尺寸允许偏差 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.2 表3 Glass fiber and magnesium cement board | |||
| 7 | 7 | 厚度尺寸允许偏差 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.2 表3 Glass fiber and magnesium cement board | |||
| 8 | 8 | 对角线差 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.2 表3 Glass fiber and magnesium cement board | |||
| 9 | 9 | 抗折强度 | 100102 | 《玻镁平板》GB/T33544-2017 5.2.3.1 表4 Glass fiber and magnesium cement board | |||
| 10 | 10 | 抗冲击强度 | 100102 | 《玻镁平板》GB/T33544-2017 5.2.3.1 表4 Glass fiber and magnesium cement board | |||
| 11 | 11 | 表观密度偏差 | 100101 | 《玻镁平板》GB/T33544-2017 5.2.3.2 Glass fiber and magnesium cement board | |||
| 12 | 12 | 出厂含水率 | 100101 | 《玻镁平板》GB/T33544-2017 5.2.3.3 Glass fiber and magnesium cement board | |||
| 13 | 13 | 干缩率 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.3.4 Glass fiber and magnesium cement board | |||
| 14 | 14 | 湿胀率 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.3.5 Glass fiber and magnesium cement board | |||
| 15 | 15 | 握螺钉力 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.3.6 表5 Glass fiber and magnesium cement board | |||
| 16 | 16 | 氯离子含量 | 100103 | 《玻镁平板》GB/T33544-2017 5.2.3.7 Glass fiber and magnesium cement board | |||
| 17 | 17 | 可浸出氯离子含量 | 100103 | 《玻镁平板》GB/T33544-2017 5.2.3.8 Glass fiber and magnesium cement board | |||
| 18 | 18 | 抗返卤性 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.3.9 Glass fiber and magnesium cement board | |||
| 19 | 19 | 不燃性 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.4 Glass fiber and magnesium cement board 引用方法:GB 8624《建筑材料及制品燃烧性能分级》 | |||
| 20 | 20 | 甲醛释放量 | 100199 | 《玻镁平板》GB/T33544-2017 5.2.5 Glass fiber and magnesium cement board 引用方法:GB18580《室内装饰装修材料人造板及其制品中甲醛释放限量》 | |||
| 21 | 21 | 放射性核素限量(内照射指数IRa) | 100199 | 《玻镁平板》GB/T33544-2017 5.2.6 Glass fiber and magnesium cement board 引用方法:GB6566《建筑材料放射性核素限量》 | |||
| 22 | 22 | 放射性核素限量(外照射指数Iγ) | 100199 | 《玻镁平板》GB/T33544-2017 5.2.6 Glass fiber and magnesium cement board 引用方法:GB6566《建筑材料放射性核素限量》 | |||