| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 种植屋面用耐根穿刺防水卷材 | 1 | 厚度 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 6.1 Waterproofing sheets of resistance to root penetration for green roof 引用方法:GB 18242—2008 或 GB 18243—2008 | ||
| 2 | 2 | 芯层厚度 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 6.1 Waterproofing sheets of resistance to root penetration for green roof 引用方法:GB/T 18173.1—2012《高分子防水材料 第1部分:片材》 | |||
| 3 | 3 | 耐霉菌腐蚀性(防霉等级) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 6.3 Waterproofing sheets of resistance to root penetration for green roof 引用方法:GB/T 1741—2007 中 5.3.3 | |||
| 4 | 4 | 接缝剥离强度(无处理) | 101402 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 6.3 Waterproofing sheets of resistance to root penetration for green roof 引用方法:GB/T 328.20《建筑防水卷材试验方法 第20部分:沥青防水卷材 接缝剥离强度》 | |||
| 5 | 5 | 接缝剥离强度(热老化处理后保持率) | 101402 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 6.3 Waterproofing sheets of resistance to root penetration for green roof | |||
| 6 | 6 | 耐根穿刺性能 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 6.4 Waterproofing sheets of resistance to root penetration for green roof | |||
| 7 | 7 | 电导率 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.5、A.4.8、A.6.1 Waterproofing sheets of resistance to root penetration for green roof | |||
| 8 | 8 | pH值 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.5、A.6.1 Waterproofing sheets of resistance to root penetration for green roof | |||
| 9 | 9 | 氯化物含量 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.6.1 Waterproofing sheets of resistance to root penetration for green roof | |||
| 10 | 10 | 氮(N) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.6.2 Waterproofing sheets of resistance to root penetration for green roof | |||
| 11 | 11 | 磷(P) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.6.2 Waterproofing sheets of resistance to root penetration for green roof | |||
| 12 | 12 | 钾(K) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.6.2 Waterproofing sheets of resistance to root penetration for green roof | |||
| 13 | 13 | 重碳酸盐(HCO3) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.8 Waterproofing sheets of resistance to root penetration for green roof | |||
| 14 | 14 | 硫酸盐(SO4) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.8 Waterproofing sheets of resistance to root penetration for green roof | |||
| 15 | 15 | 氯化物(Cl) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.8 Waterproofing sheets of resistance to root penetration for green roof | |||
| 16 | 16 | 钠(Na) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.8 Waterproofing sheets of resistance to root penetration for green roof | |||
| 17 | 17 | 硝酸盐(NO3) | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.4.8 Waterproofing sheets of resistance to root penetration for green roof | |||
| 18 | 18 | 氮 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.6.1 Waterproofing sheets of resistance to root penetration for green roof | |||
| 19 | 19 | 磷 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.6.1 Waterproofing sheets of resistance to root penetration for green roof | |||
| 20 | 20 | 钾 | 101499 | 《种植屋面用耐根穿刺防水卷材》GB/T35468-2017 A.6.1 Waterproofing sheets of resistance to root penetration for green roof | |||