| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 装配式玻纤增强无机材料复合保温墙体技术要求 | 1 | 板面漏筋纤、飞边毛刺 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.1 表2 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | ||
| 2 | 2 | 板面泛霜 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.1 表2 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 3 | 3 | 面层与夹芯层粘结处有裂缝 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.1 表2 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 4 | 4 | 板面裂缝 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.1 表2 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 5 | 5 | 缺棱掉角 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.1 表2 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 6 | 6 | 宽度(尺寸允许偏差) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 7 | 7 | 高度(尺寸允许偏差) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 8 | 8 | 厚度(尺寸允许偏差) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 9 | 9 | 对角线差 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 10 | 10 | 表面平整度 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 11 | 11 | 侧向弯曲 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 12 | 12 | 翘曲 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 13 | 13 | 墙体挂件中心位置(螺栓连接) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 14 | 14 | 墙体挂件中心位置(焊接) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 15 | 15 | 洞口宽度、高度 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 16 | 16 | 洞口对角线差 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.2 表3 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 17 | 17 | 耐撞击性能 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.3 表4 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 18 | 18 | 耐火极限 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.3 表4 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 19 | 19 | 空气声隔声性能(Rw+C) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.3 表4 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials | |||
| 20 | 20 | 抗风压性能 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.3 表4 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 31433—2015《建筑幕墙、门窗通用技术条件》 | |||
| 21 | 21 | 水密性能 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.3 表4 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 31433—2015《建筑幕墙、门窗通用技术条件》 | |||
| 22 | 22 | 气密性能 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.3 表4 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 31433—2015《建筑幕墙、门窗通用技术条件》 | |||
| 23 | 23 | 层间变形性能 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.3 表4 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 18250—2015《建筑幕墙层间变形性能分级及检测方法》 | |||
| 24 | 24 | 拉伸粘结强度(原强度) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.4 表5 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 287—2013 中 6.4.3 | |||
| 25 | 25 | 拉伸粘结强度(耐水强度) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.4 表5 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 287—2013 中 6.4.3 | |||
| 26 | 26 | 拉伸粘结强度(耐冻融强度) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.4 表5 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 287—2013 中 6.4.3 | |||
| 27 | 27 | 干燥收缩值 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.4 表5 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 30100—2013 中 14.3.1 | |||
| 28 | 28 | 放射性(内照射指数 I_Ra) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.4 表5 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB 6566《建筑材料放射性核素限量》 | |||
| 29 | 29 | 放射性(外照射指数 I_γ) | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.4 表5 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB 6566《建筑材料放射性核素限量》 | |||
| 30 | 30 | 甲醛释放量 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 6.4 表5 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB 18580《室内装饰装修材料 人造板及其制品中甲醛释放限量》 | |||
| 31 | 31 | 表观密度 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 15231《玻璃纤维增强水泥性能试验方法》 | |||
| 32 | 32 | 吸水率 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 15231《玻璃纤维增强水泥性能试验方法》 | |||
| 33 | 33 | 不透水性 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 7019《纤维水泥制品试验方法》 | |||
| 34 | 34 | 湿度变形 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 396-2012 | |||
| 35 | 35 | 饱水状态抗折强度 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 396-2012 | |||
| 36 | 36 | 抗冲击性 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 396-2012 | |||
| 37 | 37 | 抗冻性 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 396-2012 | |||
| 38 | 38 | 耐热雨性能 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 396-2012 | |||
| 39 | 39 | 耐热水性能 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 396-2012 | |||
| 40 | 40 | 耐干湿性能 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:JG/T 396-2012 | |||
| 41 | 41 | 燃烧性能等级 | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB/T 5464《建筑材料不燃性试验方法》 | |||
| 42 | 42 | 放射性-内照射指数IRa | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB 6566《建筑材料放射性核素限量》 | |||
| 43 | 43 | 放射性-外照射指数Iγ | 082399 | 《装配式玻纤增强无机材料复合保温墙体技术要求》GB/T36140-2018 表B.1 Technical requirements for assembled insulation combination wall composite by glass fiber reinforced inorganic materials 引用方法:GB 6566《建筑材料放射性核素限量》 | |||