| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管 | 1 | 弯曲度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.1.5、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:QB/T 2803《硬质塑料管材弯曲度测定方法》 | |||
| 2 | 2 | 受压开裂稳定性 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.1.6、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 3 | 3 | 纵向尺寸回缩率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.1.7、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 6671《热塑性塑料管材 纵向回缩率的测定》 | ||||
| 4 | 4 | 强度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.1.8、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 6111;GB/T 15560 | ||||
| 5 | 5 | 热稳定性 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.1.9、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 17391《聚乙烯管材与管件热稳定性试验方法》 | ||||
| 6 | 6 | 熔体质量流动速率变化值 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.1.10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 3682.1《塑料 热塑性塑料熔体质量流动速率(MFR)和熔体体积流动速率(MVR)的测定第1部分:标准方法》 | ||||
| 7 | 7 | 熔体质量流动速率变化率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.1.10、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 3682.1《塑料 热塑性塑料熔体质量流动速率(MFR)和熔体体积流动速率(MVR)的测定第1部分:标准方法》 | ||||
| 8 | 8 | 透氧率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.1.11、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:ISO 17455《塑料管道系统 多层管 阻隔层氧气渗透性能的测定(Plastics piping systems—Multylayer pipes—Determination of the oxygen permeability of the barrier pipe)》 | ||||
| 9 | 9 | 外观 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.1、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 10 | 10 | 管材端面角度偏差 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.1 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 11 | 11 | 最小壁厚 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.2 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 8806《塑料管道系统 塑料部件尺寸的测定》 | ||||
| 12 | 12 | 密度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.3、6.3.1、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 1033.1《塑料 非泡沫塑料密度的测定 第1部分:浸渍法、液体比重瓶法和滴定法》 | ||||
| 13 | 13 | 纵向回缩率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.4、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 6671《热塑性塑料管材 纵向回缩率的测定》 | ||||
| 14 | 14 | 拉伸屈服强度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.5、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 8804.3《热塑性塑料管材 拉伸性能测定 第3部分:聚烯烃管材》 | ||||
| 15 | 15 | 断裂伸长率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.6、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 8804.3《热塑性塑料管材 拉伸性能测定 第3部分:聚烯烃管材》 | ||||
| 16 | 16 | 氧化诱导时间 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.7 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 17391《聚乙烯管材与管件热稳定性试验方法》 | ||||
| 17 | 17 | 耐环境应力开裂失效时间 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.8 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 18 | 18 | 长期机械性能最短破坏时间 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.2.9 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 19 | 19 | 闭孔率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.2、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 10799《硬质泡沫塑料 开孔和闭孔体积百分率的测定》 | ||||
| 20 | 20 | 泡孔平均尺寸 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.3 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 21 | 21 | 吸水率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.4、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 22 | 22 | 导热系数 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.5、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 10297《非金属固体材料导热系数的测定 热线法》 | ||||
| 23 | 23 | 压缩强度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.6、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 24 | 24 | 空洞和气泡面积总和占比 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.7 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 25 | 25 | 单个空洞尺寸 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.7 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 26 | 26 | 尺寸变化率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.8 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 27 | 27 | 质量变化率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.8 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 28 | 28 | 强度增长率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.8 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 29 | 29 | 保温层最小厚度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.3.9 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 30 | 30 | 轴向剪切强度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.4.1、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 31 | 31 | 保温层挤压变形量 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.4.2、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 32 | 32 | 外护管划痕深度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.4.3、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 33 | 33 | 工作管端头预留尺寸L | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.4.4 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 34 | 34 | 外护管外径增大率 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.4.5、表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 35 | 35 | 报警线电阻值 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.4.6 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 36 | 36 | 最大轴线偏心距 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 6.4.7 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 37 | 37 | 规格、尺寸及偏差 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 38 | 38 | 不圆度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 39 | 39 | 增强钢带厚度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 40 | 40 | 规格、尺寸 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 41 | 41 | 耐环境应力开裂 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 42 | 42 | 长期机械性能 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 43 | 43 | 泡孔尺寸 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 44 | 44 | 空洞、气泡 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 45 | 45 | 耐热性 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 46 | 46 | 保温层厚度 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 47 | 47 | 工作管端头预留尺寸 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 48 | 48 | 报警线 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||
| 49 | 49 | 轴线偏心距 | 《高密度聚乙烯外护管聚氨酯发泡预制直埋保温钢塑复合管》GB/T37263-2018 表10 Prefabricated directly buried insulating plastic-steel-plastic composite pipes with polyurethane(PUR) foamed-plastics and high density polyethylene(PE) casing pipes | ||||