| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 微机电系统(MEMS)技术 MEMS 器件的可靠性综合 | 1 | 预处理试验 | 040101 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.1.4.3 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments | ||
| 2 | 2 | 高温工作试验 | 040101 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.2.1.4.2 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments | |||
| 3 | 3 | 高温贮存试验 | 040110 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.2.2.3.2 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments | |||
| 4 | 4 | 低温贮存试验 | 040110 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.2.3.3.2 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments | |||
| 5 | 5 | 温度循环试验 | 040101 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.2.4.4.2 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments | |||
| 6 | 6 | 恒定湿热加速试验 | 040103 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.2.5.1、4.2.5.4.2 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments 引用方法:GB/T 2423.3—2016 | |||
| 7 | 7 | 高压湿热试验 | 040103 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.2.6.4.2 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments | |||
| 8 | 8 | 机械冲击试验 | 040105 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.3.1.4.3 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments 引用方法:GJB 548A-96 方法2002A(表8未包括的条件) | |||
| 9 | 9 | 随机机械振动试验 | 040107 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.3.2.4.3 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments | |||
| 10 | 10 | 湿热-冲击耦合试验 | 040121 | 《微机电系统(MEMS)技术 MEMS 器件的可靠性综合环境试验方法》GB/T38341-2019 4.4.1.4.3 Micro-electromechanical system technology— The reliability test methods of MEMS in integrated environments | |||