| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 金属材料 | 1 | 扩散角误差 | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.10.2.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | ||
| 2 | 2 | 副瓣幅度(反射方式) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.10.2.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 3 | 3 | 副瓣幅度(电磁声方式) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.10.2.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 4 | 4 | 焦距误差 | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.10.3.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 5 | 5 | 焦区宽度误差 | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.10.4.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 6 | 6 | 焦区长度误差 | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.10.5.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 7 | 7 | 入射点误差 | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.2.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 8 | 8 | 声束角误差(频率低于2 MHz) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.3.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 9 | 9 | 声束角误差(频率不低于2 MHz) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.3.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 10 | 10 | 扩散角误差(斜入射) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.3.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 11 | 11 | 副瓣幅度(反射方法,标称声束角45°~65°) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.3.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 12 | 12 | 副瓣幅度(反射方法,标称声束角较大) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.3.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 13 | 13 | 副瓣幅度(电磁声接收器,标称声束角45°~65°) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.3.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 14 | 14 | 副瓣幅度(电磁声接收器,标称声束角较大) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.3.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 15 | 15 | 焦距误差(斜入射) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.4.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 16 | 16 | 焦区宽度误差(斜入射) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.5.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 17 | 17 | 焦区长度误差(斜入射) | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.11.6.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 18 | 18 | 近场长度 | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.13.2 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||
| 19 | 19 | 三维辐射声场分布 | 110199 | 《无损检测 电磁声换能器(EMATs)指南》GB/T38895-2020 7.12.3 Non-destructive testing—Guidelines for electromagnetic acoustic transducers (EMATs) | |||