| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 高密度聚乙烯无缝外护管 预制直埋保温管件 | 1 | 弯曲部分椭圆度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.1.2.4、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | |||
| 2 | 2 | 弯曲半径 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.1.2.5、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 3 | 3 | 弯曲角度允许偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.1.2.6 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 4 | 4 | 直管段长度及偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.1.2.7、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 5 | 5 | T型三通支管与主管垂直角度偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.1.3.3 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 6 | 6 | 异径管两端直管段长度及偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.1.4.2、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 7 | 7 | 焊缝无损检测抽检比例(射线检测) | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.1.5.4 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:NB/T 47013.2—2015《承压设备无损检测 第2部分:射线检测》 | ||||
| 8 | 8 | 焊缝无损检测抽检比例(超声波检测) | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.1.5.4 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:NB/T 47013.3—2015《承压设备无损检测 第3部分:超声检测》 | ||||
| 9 | 9 | 聚乙烯树脂密度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.1.2 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 10 | 10 | 炭黑密度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.1.2 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 11 | 11 | 炭黑甲苯萃取量 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.1.2 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 12 | 12 | 炭黑平均颗粒尺寸 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.1.2 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 13 | 13 | 炭黑结块、气泡、空洞或杂质尺寸 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.1.3 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 14 | 14 | 炭黑含量 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.1.4、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 15 | 15 | 熔体质量流动速率(MFR) | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.1.5 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 16 | 16 | 氧化诱导时间(210℃) | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.1.6 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 17 | 17 | 外护管件外观 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.1 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 18 | 18 | 密度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.2、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 19 | 19 | 拉伸屈服强度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.3 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 20 | 20 | 断裂伸长率 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.3 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 21 | 21 | 纵向回缩率 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.4、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 22 | 22 | 耐环境应力开裂失效时间 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.5 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 23 | 23 | 长期力学性能(拉应力4MPa下最短破坏时间) | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.6 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 24 | 24 | 最小壁厚 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.7 a) 表7 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 25 | 25 | 平均外径公差(Dcm-Dc) | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.7 b) 公式(2) Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 26 | 26 | 公称壁厚与任一点壁厚偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.7 c) 公式(3) Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 27 | 27 | 外护弯头(弯管)直管段长度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.8 表8 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 28 | 28 | T型三通外护支管拔制高度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.9 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 29 | 29 | 加强焊接带状套筒尺寸 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.10 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 30 | 30 | 椭圆度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.11 公式(4) Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 31 | 31 | 弯头与弯管角度偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.2.2.12、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 32 | 32 | 平均泡孔尺寸 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.3.2、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 33 | 33 | 空洞和气泡面积占比 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.3.3 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 34 | 34 | 保温层密度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.3.4 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 35 | 35 | 径向压缩强度或10%相对形变压缩应力 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.3.5 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 36 | 36 | 吸水率 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.3.6、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 37 | 37 | 闭孔率 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.3.7、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 38 | 38 | 导热系数λ50 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.3.8 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 39 | 39 | 外护管件表面温度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.3.9 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 40 | 40 | 保温管件管端角度误差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.1 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 41 | 41 | 保温层受挤压径向变形量 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.2 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 42 | 42 | 外护管件划痕深度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.2 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 43 | 43 | 焊接预留段长度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.3 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 44 | 44 | 发泡后保温管件外径 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.4 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29047《高密度聚乙烯外护管硬质聚氨酯泡沫塑料预制直埋保温管及管件》 | ||||
| 45 | 45 | 钢制管件中心线与外护管中心线角度偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.5 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 46 | 46 | 最大轴线偏心距 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.6 表9 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 47 | 47 | 弯头、弯管最小保温层厚度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.8 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 48 | 48 | 信号线电阻值 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.9 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:CJJ/T 254 | ||||
| 49 | 49 | 主要尺寸允许偏差H | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.10 表10 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 50 | 50 | 主要尺寸允许偏差L | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.10 表10 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 51 | 51 | 预期寿命与长期耐温性 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.11、表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29047《高密度聚乙烯外护管硬质聚氨酯泡沫塑料预制直埋保温管及管件》 | ||||
| 52 | 52 | 低温冲击(-20°C落锤冲击) | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.12 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29046《城镇供热预制直埋保温管道技术指标检测方法》 | ||||
| 53 | 53 | 耐高温蠕变性能 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 5.4.13 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe 引用方法:GB/T 29047《高密度聚乙烯外护管硬质聚氨酯泡沫塑料预制直埋保温管及管件》 | ||||
| 54 | 54 | 材质、尺寸公差及性能 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 55 | 55 | 公称尺寸及壁厚 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 56 | 56 | 外观 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 57 | 57 | 弯曲部分外观 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 58 | 58 | 弯曲部分最小壁厚 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 59 | 59 | 弯曲角度偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 60 | 60 | T型三通支管与主管角度偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 61 | 61 | 焊缝质量 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 62 | 62 | 强度和气密性 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 63 | 63 | 炭黑弥散度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 64 | 64 | 熔体质量流动速率 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 65 | 65 | 热稳定性 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 66 | 66 | 拉伸屈服强度与断裂伸长率 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 67 | 67 | 耐环境应力开裂 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 68 | 68 | 长期力学性能 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 69 | 69 | 外径和最小壁厚 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 70 | 70 | 直管段长度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 71 | 71 | T型三通支管拔制高度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 72 | 72 | T型三通加强焊缝 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 73 | 73 | 空洞和气泡 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 74 | 74 | 压缩强度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 75 | 75 | 导热系数 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 76 | 76 | 保温层厚度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 77 | 77 | 管端垂直度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 78 | 78 | 挤压变形及划痕 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 79 | 79 | 管端焊接预留段长度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 80 | 80 | 外护管外径 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 81 | 81 | 钢制管件与外护管角度偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 82 | 82 | 轴线偏心距 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 83 | 83 | T型三通和外护管配合尺寸 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 84 | 84 | 最小保温层厚度 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 85 | 85 | 信号线 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 86 | 86 | 主要尺寸允许偏差 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 87 | 87 | 抗冲击性 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||
| 88 | 88 | 蠕变性能 | 《高密度聚乙烯无缝外护管 预制直埋保温管件》GB/T39246-2020 表11 Prefabricated directly buried insulating fittings with seamless high density polyethylene casing pipe | ||||