| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 刻蚀机用硅电极及硅环 | 1 | 导电类型(掺杂剂) | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.1 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 1550《非本征半导体材料导电类型测试方法》 | |||
| 2 | 2 | 电阻率 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.1 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 1551 直排四探针法 | ||||
| 3 | 3 | 径向电阻率变化 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.1 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 11073《硅片径向电阻率变化的测量方法》 | ||||
| 4 | 4 | 直径及允许偏差 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 5 | 5 | 厚度允许偏差 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 6 | 6 | 平面度 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 7 | 7 | 定位孔直径允许偏差 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 8 | 8 | 倒角长度及允许偏差 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 9 | 9 | 微孔直径及允许偏差 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 10 | 10 | 内径允许偏差 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 11 | 11 | 同心度 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 12 | 12 | 垂直度 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.2 Silicon electrode and silicon ring for plasma etching machine | ||||
| 13 | 13 | 晶向及晶向偏离度 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.3 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 1555《半导体单晶晶向测定方法》 | ||||
| 14 | 14 | 间隙氧含量 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.4 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 1557《硅晶体中间隙氧含量的红外吸收测量方法》 | ||||
| 15 | 15 | 代位碳含量 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.5 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 1558《硅中代位碳原子含量红外吸收测量方法》 | ||||
| 16 | 16 | 晶体缺陷 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.6 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 1554《硅晶体完整性化学择优腐蚀检验方法》 | ||||
| 17 | 17 | 表面粗糙度(Ra) | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.7 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 29505《硅片平坦表面的表面粗糙度测量方法》 | ||||
| 18 | 18 | 表面质量 | 《刻蚀机用硅电极及硅环》GB/T41652-2022 4.8 Silicon electrode and silicon ring for plasma etching machine 引用方法:GB/T 6624《硅抛光片表面质量目测检验方法》 | ||||