| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 集成电路金属封装外壳质量技术要求 | 1 | 引线和壳体镀层厚度 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 4.2 Quality and technical requirements for metal packages used for integrated circuits 引用方法:SJ 20129 | ||
| 2 | 2 | 绝缘电阻 | 040601 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 4.4.2 Quality and technical requirements for metal packages used for integrated circuits | |||
| 3 | 3 | 破开的表面气泡直径 | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.1 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 4 | 4 | 破开的表面气泡或内部气泡聚集成团覆盖引线和孔壁间距L的比例 | 040613 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.1 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 5 | 5 | 内部气泡连成一线覆盖引线和孔壁间距L的比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.1 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 6 | 6 | 多个内部气泡面积占绝缘子面积的比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.1 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 7 | 7 | 单个内部气泡覆盖引线和孔壁间距L的比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.1 e) Quality and technical requirements for metal packages used for integrated circuits | |||
| 8 | 8 | 陶瓷绝缘子裂纹 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 9 | 9 | 圆弧状裂纹超出象限角度 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 10 | 10 | 径向裂纹超出弯月区 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 11 | 11 | 非从引线开始产生的径向裂纹 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 12 | 12 | 从引线开始延伸至弯月区平均低点之外的径向裂纹条数 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 e) Quality and technical requirements for metal packages used for integrated circuits | |||
| 13 | 13 | 同一象限内从引线开始延伸至弯月区平均低点之外的径向裂纹条数 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 f) Quality and technical requirements for metal packages used for integrated circuits | |||
| 14 | 14 | 绝缘子表面龟裂 | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 g) Quality and technical requirements for metal packages used for integrated circuits | |||
| 15 | 15 | 玻璃缺损导致引线上基底金属裸露深度H | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 h) Quality and technical requirements for metal packages used for integrated circuits | |||
| 16 | 16 | 玻璃缺损面积占引线和外壳间绝缘子距离L的比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.2 i) Quality and technical requirements for metal packages used for integrated circuits | |||
| 17 | 17 | 绝缘子爬高H | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.3 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 18 | 18 | 绝缘子爬高形状 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.3 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 19 | 19 | 绝缘子浸润/反弯月形 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.3 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 20 | 20 | 绝缘子剩余厚度h与壳体厚度H之比 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.3 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 21 | 21 | 绝缘子外溢距离L | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.3 e) Quality and technical requirements for metal packages used for integrated circuits | |||
| 22 | 22 | 绝缘子外溢距离占两相邻绝缘子间金属长度W的比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.3 e) Quality and technical requirements for metal packages used for integrated circuits | |||
| 23 | 23 | 接插台面/圆形外壳/墙体式外壳内部底板上绝缘子飞溅物 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.3 f) Quality and technical requirements for metal packages used for integrated circuits | |||
| 24 | 24 | 外墙体上绝缘子飞溅物直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.3 g) Quality and technical requirements for metal packages used for integrated circuits | |||
| 25 | 25 | 绝缘子表面嵌入式异物或夹杂物导致绝缘电阻 | 040601 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.4 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 26 | 26 | 嵌入式镀层致使引线和外壳间绝缘降低比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.4 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 27 | 27 | 利用聚合物或其他异物优化处理密封或重新处理密封 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.4 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 28 | 28 | 外壳墙体和底板外部界面焊料凹陷深度L | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.5 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 29 | 29 | 拐角处焊料凹陷超出墙体厚度比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.5 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 30 | 30 | 外壳其他部位焊料凹陷底部可见性 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.5 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 31 | 31 | 外壳墙体和底板界面焊料不连续且孔隙底部不可见 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.5 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 32 | 32 | 海绵状焊料凹坑直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.6 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 33 | 33 | 焊料分离或剥落 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.6 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 34 | 34 | 钎焊外壳墙体和底板未对准导致超出整体最大外部尺寸 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.6 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 35 | 35 | 焊料边缘流出厚度 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.7 Quality and technical requirements for metal packages used for integrated circuits | |||
| 36 | 36 | 直头引线焊料爬高 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.8 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 37 | 37 | 钉头引线顶面焊料 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.8 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 38 | 38 | 键合区或关键密封区焊料 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.8 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 39 | 39 | 焊料过多增加引线直径超出最大直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.8 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 40 | 40 | 陶瓷密封处修补或返工过多焊料 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.8 e) Quality and technical requirements for metal packages used for integrated circuits | |||
| 41 | 41 | 钉头接地线钉头悬在焊颈上 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.8 f) Quality and technical requirements for metal packages used for integrated circuits | |||
| 42 | 42 | 扁平引线表面缺陷面积占横截面积比例 | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 43 | 43 | 扁平引线表面缺陷深度 | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 44 | 44 | 扁平引线表面缺陷直径 | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 45 | 45 | 扁平引线内部键合区引线可见缺陷 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 46 | 46 | 圆引线连续键合面积(顶部)比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 47 | 47 | 圆引线缺陷导致引线直径减小 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 48 | 48 | 基底金属裸露面积占引线表面非键合区比例 | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 e) Quality and technical requirements for metal packages used for integrated circuits | |||
| 49 | 49 | 键合区引线凸起伸出高度h | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 f) Quality and technical requirements for metal packages used for integrated circuits | |||
| 50 | 50 | 扁平引线凸起增加直径或宽度超出最大值的比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 g) Quality and technical requirements for metal packages used for integrated circuits | |||
| 51 | 51 | 圆引线凸起增加引线直径超出最大直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 g) Quality and technical requirements for metal packages used for integrated circuits | |||
| 52 | 52 | 悬挂的引线凸起可随探针移动 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.9 h) Quality and technical requirements for metal packages used for integrated circuits | |||
| 53 | 53 | 扁平引线连续键合区比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.10 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 54 | 54 | 扁平引线表面镀层粗糙度Ra | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.10 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 55 | 55 | 圆引线(直径≥0.46mm)连续键合区比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.10 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 56 | 56 | 圆引线(直径≥0.46mm)连续键合区直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.10 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 57 | 57 | 圆引线表面镀层粗糙度Ra | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.10 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 58 | 58 | 圆引线(直径<0.46mm)连续键合区比例 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.10 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 59 | 59 | 引线异物或其他附着物 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.10 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 60 | 60 | 引线镀层起皮或剥落 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.10 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 61 | 61 | 偏心引线距离h(孔直径d≥0.84mm) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 62 | 62 | 偏心引线距离h(孔直径d<0.84mm) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 63 | 63 | 引线中心与外壳封孔中心同轴范围 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 64 | 64 | 内引线倾斜距离h(L≤0.90mm) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 65 | 65 | 内引线倾斜角度θ(L≤0.90mm) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 66 | 66 | 内引线倾斜距离h(L>0.90mm) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 67 | 67 | 内引线倾斜角度θ(L>0.90mm) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 68 | 68 | 内引线弯曲或弯折距离h | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 69 | 69 | 外引线弯曲或弯折角度θ | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.11 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 70 | 70 | 熔焊外壳关键盖板密封区缺陷深度(占熔筋焊比例) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 71 | 71 | 熔焊外壳关键盖板密封区缺陷直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 72 | 72 | 其他外壳类型关键密封区缺陷深度 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 73 | 73 | 其他外壳类型关键密封区缺陷直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 74 | 74 | 基板区缺陷深度 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 75 | 75 | 基板区缺陷直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 76 | 76 | 普通区域缺陷深度 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 77 | 77 | 普通区域缺陷直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 78 | 78 | 关键密封区固体凸起伸出量 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 g) Quality and technical requirements for metal packages used for integrated circuits | |||
| 79 | 79 | 基板区或芯片黏接区固体凸起伸出量 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 h) Quality and technical requirements for metal packages used for integrated circuits | |||
| 80 | 80 | 外壳底部(安装面)固体凸起伸出量 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 i) Quality and technical requirements for metal packages used for integrated circuits | |||
| 81 | 81 | 其他普通区域固体凸起伸出量 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.12 j) Quality and technical requirements for metal packages used for integrated circuits | |||
| 82 | 82 | 外壳普通表面表面粗糙度Ra | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.13 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 83 | 83 | 机加工外壳表面台阶 | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.13 d) Quality and technical requirements for metal packages used for integrated circuits | |||
| 84 | 84 | 熔焊盖板关键盖板密封区缺陷深度(占熔焊比例) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.14 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 85 | 85 | 熔焊盖板关键盖板密封区缺陷直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.14 a) Quality and technical requirements for metal packages used for integrated circuits | |||
| 86 | 86 | 盖板关键密封区缺陷深度 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.14 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 87 | 87 | 盖板关键密封区缺陷直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.14 b) Quality and technical requirements for metal packages used for integrated circuits | |||
| 88 | 88 | 盖板普通区域缺陷深度(占材料厚度比例) | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.14 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 89 | 89 | 盖板普通区域缺陷直径 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.14 c) Quality and technical requirements for metal packages used for integrated circuits | |||
| 90 | 90 | 盖板关键密封区固体凸起伸出量 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.14 e) Quality and technical requirements for metal packages used for integrated circuits | |||
| 91 | 91 | 盖板其他普通区域固体凸起伸出量 | 040699 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.14 f) Quality and technical requirements for metal packages used for integrated circuits | |||
| 92 | 92 | 盖板表面表面粗糙度Ra | 040615 | 《集成电路金属封装外壳质量技术要求》GB/T43538-2023 B.1.15 c) Quality and technical requirements for metal packages used for integrated circuits | |||