| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 高密度互连印制板分规范 | 1 | 最小刚性介质层厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.1.1 Sectional specification for high density interconnect printed boards | |||
| 2 | 2 | 挠性介质厚度公差 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.1.1 Sectional specification for high density interconnect printed boards | ||||
| 3 | 3 | 积层介质被蚀厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.1.2 Sectional specification for high density interconnect printed boards | ||||
| 4 | 4 | 孔内材料填充率 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.2 Sectional specification for high density interconnect printed boards | ||||
| 5 | 5 | 孔内填充材料表面凹陷和凸起 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.2 Sectional specification for high density interconnect printed boards | ||||
| 6 | 6 | 刚性区层压空洞尺寸 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.3 Sectional specification for high density interconnect printed boards | ||||
| 7 | 7 | 挠性区粘结空洞尺寸 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.3 Sectional specification for high density interconnect printed boards | ||||
| 8 | 8 | 层压裂缝长度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.4 Sectional specification for high density interconnect printed boards | ||||
| 9 | 9 | 树脂凹缩最大深度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.6 Sectional specification for high density interconnect printed boards | ||||
| 10 | 10 | 树脂凹缩占基材累积厚度比例 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.2.6 Sectional specification for high density interconnect printed boards | ||||
| 11 | 11 | 电镀锡铅(非热熔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 12 | 12 | 板边连接器及非焊接区镀金层最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 13 | 13 | 焊接区镀金层最大厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 14 | 14 | 金属丝键合区镀金层(超声波压焊)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 15 | 15 | 金属丝键合区镀镍底层(超声波压焊)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 16 | 16 | 金属丝键合区镀金层(热压焊)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 17 | 17 | 金属丝键合区镀镍底层(热压焊)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 18 | 18 | 板边连接器镀镍层最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 19 | 19 | 防止形成铜锡合金的镍阻挡层最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 20 | 20 | 化学浸镍最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 21 | 21 | 化学浸金最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 22 | 22 | 化学镍层厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 23 | 23 | 化学钯层厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 24 | 24 | 化学金层厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 25 | 25 | 表面和孔内铜(镀覆孔、盲孔、大于2层的埋孔,不含微导通孔)平均厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 26 | 26 | 表面和孔内铜(镀覆孔、盲孔、大于2层的埋孔,不含微导通孔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 27 | 27 | 表面和孔内铜(2层的埋孔)平均厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 28 | 28 | 表面和孔内铜(2层的埋孔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 29 | 29 | 包覆铜(镀覆孔、盲孔、大于2层的埋孔,不含微导通孔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 30 | 30 | 包覆铜(2层的埋孔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 31 | 31 | 表面和孔内铜(镀覆孔,板厚小于1.5mm,不含Tg小于110°C材料)平均厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 32 | 32 | 表面和孔内铜(镀覆孔,板厚大于1.5mm,含Tg小于110°C材料)平均厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 33 | 33 | 表面和孔内铜(镀覆孔,板厚大于1.5mm,含Tg小于110°C材料)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 34 | 34 | 表面和孔内铜(盲孔、大于2层的埋孔,不含微导通孔)平均厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 35 | 35 | 表面和孔内铜(盲孔、大于2层的埋孔,不含微导通孔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 36 | 36 | 表面和孔内铜(2层的埋孔)平均厚度(2类3类) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 37 | 37 | 表面和孔内铜(2层的埋孔)最小厚度(2类3类) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 38 | 38 | 包覆铜(盲孔、大于2层的埋孔,不含微导通孔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 39 | 39 | 包覆铜(2层的埋孔)最小厚度(2类3类) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 40 | 40 | 表面和孔内铜(微导通孔)平均厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 41 | 41 | 表面和孔内铜(微导通孔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 42 | 42 | 包覆铜(微导通孔)最小厚度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.1 表1 Sectional specification for high density interconnect printed boards | ||||
| 43 | 43 | 外层导电图形最小铜箔厚度(1类印制板) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.1 表2 Sectional specification for high density interconnect printed boards | ||||
| 44 | 44 | 1级和2级加电镀层(20μm)后的最小铜箔厚度(1类印制板) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.1 表2 Sectional specification for high density interconnect printed boards | ||||
| 45 | 45 | 3级加电镀层(25μm)后的最小铜箔厚度(1类印制板) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.1 表2 Sectional specification for high density interconnect printed boards | ||||
| 46 | 46 | 内层铜箔厚度(标称5.1μm) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 47 | 47 | 内层铜箔厚度(标称8.5μm) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 48 | 48 | 内层铜箔厚度(标称12.0μm) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 49 | 49 | 内层铜箔厚度(标称17.1μm) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 50 | 50 | 内层铜箔厚度(标称34.3μm) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 51 | 51 | 内层铜箔厚度(标称68.6μm) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 52 | 52 | 内层铜箔厚度(标称102.9μm) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 53 | 53 | 内层铜箔厚度(标称137.2μm) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 54 | 54 | 内层铜箔厚度(标称137.2μm以上) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.2.2 表4 Sectional specification for high density interconnect printed boards | ||||
| 55 | 55 | 导通孔内层环宽(1级、2级,未填角/泪滴盘设计) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.3.1 b) Sectional specification for high density interconnect printed boards | ||||
| 56 | 56 | 导通孔内层环宽(3级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.3.1 c) Sectional specification for high density interconnect printed boards | ||||
| 57 | 57 | 微导通孔捕获连接盘与导体连接处环宽(2级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.3.2 b) Sectional specification for high density interconnect printed boards | ||||
| 58 | 58 | 微导通孔目标连接盘最小接触面尺寸(激光钻孔,1级、2级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.3.3 a) Sectional specification for high density interconnect printed boards | ||||
| 59 | 59 | 微导通孔目标连接盘最小接触面尺寸(激光钻孔,3级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.3.3 a) Sectional specification for high density interconnect printed boards | ||||
| 60 | 60 | 连接盘起翘(模拟返工、热应力或温度冲击试验后) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.4 Sectional specification for high density interconnect printed boards | ||||
| 61 | 61 | 侧蚀(3级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.3.5 Sectional specification for high density interconnect printed boards | ||||
| 62 | 62 | 微导通孔孔型(孔底/孔口比) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.1 Sectional specification for high density interconnect printed boards | ||||
| 63 | 63 | 微导通孔张角 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.1 Sectional specification for high density interconnect printed boards | ||||
| 64 | 64 | 铜镀层空洞数量(1级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.3 a) Sectional specification for high density interconnect printed boards | ||||
| 65 | 65 | 铜镀层空洞数量(2级、3级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.3 a) Sectional specification for high density interconnect printed boards | ||||
| 66 | 66 | 铜镀层空洞长度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.3 b) Sectional specification for high density interconnect printed boards | ||||
| 67 | 67 | 环状铜镀层空洞角度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.3 d) Sectional specification for high density interconnect printed boards | ||||
| 68 | 68 | 电镀铜填孔空洞总面积 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.4 Sectional specification for high density interconnect printed boards | ||||
| 69 | 69 | 包覆铜镀层最小延伸长度 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.5 Sectional specification for high density interconnect printed boards | ||||
| 70 | 70 | 盖覆铜镀层最小厚度(2级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.6 表5 Sectional specification for high density interconnect printed boards | ||||
| 71 | 71 | 盖覆铜镀层最小厚度(3级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.6 表5 Sectional specification for high density interconnect printed boards | ||||
| 72 | 72 | 填塞后导通孔最大凹陷(2级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.6 表5 Sectional specification for high density interconnect printed boards | ||||
| 73 | 73 | 填塞后导通孔最大凹陷(3级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.6 表5 Sectional specification for high density interconnect printed boards | ||||
| 74 | 74 | 填塞后导通孔最大凸起(2级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.6 表5 Sectional specification for high density interconnect printed boards | ||||
| 75 | 75 | 填塞后导通孔最大凸起(3级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.6 表5 Sectional specification for high density interconnect printed boards | ||||
| 76 | 76 | 外层铜箔垂直边缘界面分离最大长度(1级) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.7 c) Sectional specification for high density interconnect printed boards | ||||
| 77 | 77 | 芯吸 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.10 Sectional specification for high density interconnect printed boards | ||||
| 78 | 78 | 钉头 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.11 Sectional specification for high density interconnect printed boards | ||||
| 79 | 79 | 正凹蚀深度(内层露铜长度) | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.12.1 Sectional specification for high density interconnect printed boards | ||||
| 80 | 80 | 负凹蚀量X | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.12.2 Sectional specification for high density interconnect printed boards | ||||
| 81 | 81 | 最大凹蚀量Z | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.12.2 Sectional specification for high density interconnect printed boards | ||||
| 82 | 82 | 去钻污孔壁径向除去材料 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.13 Sectional specification for high density interconnect printed boards | ||||
| 83 | 83 | 去钻污后树脂残余 | 《高密度互连印制板分规范》GB/T43799-2024 6.6.2.4.13 Sectional specification for high density interconnect printed boards | ||||