| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 农村房屋用夹心保温轻质墙板 | 1 | 混凝土强度等级 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.1.1 表2、7.2.1.1 Lightweight sandwich insulation wall panel for rural housing | |||
| 2 | 2 | 干密度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.1.1 表2、7.2.1.1 Lightweight sandwich insulation wall panel for rural housing | ||||
| 3 | 3 | 干燥收缩值 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.1.1 表2、6.1.1.2 表3、7.2.1.1 等4处 Lightweight sandwich insulation wall panel for rural housing | ||||
| 4 | 4 | 抗冻性-质量损失 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.1.1 表2、6.1.1.2 表3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 5 | 5 | 抗冻性-强度损失 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.1.1 表2、6.1.1.2 表3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 6 | 6 | 抗压强度-平均值 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.1.2 表3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 7 | 7 | 抗压强度-单组最小值 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.1.2 表3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 8 | 8 | 面密度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.1.2 表3、7.2.1.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 9 | 9 | 导热系数(平均温度25°C) | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.2 表4 Lightweight sandwich insulation wall panel for rural housing | ||||
| 10 | 10 | 燃烧性能等级 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.2 表4、7.2.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 11 | 11 | 体积吸水率 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.2 表4、7.2.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 12 | 12 | 尺寸稳定性(70°C,48h) | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.2 表4 Lightweight sandwich insulation wall panel for rural housing | ||||
| 13 | 13 | 拉伸强度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.3.1、6.1.3.2、6.1.3.3 Lightweight sandwich insulation wall panel for rural housing 引用方法:JG/T 561 | ||||
| 14 | 14 | 拉伸弹性模量 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.3.1、6.1.3.2 Lightweight sandwich insulation wall panel for rural housing 引用方法:JG/T 561 | ||||
| 15 | 15 | 层间剪切强度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.3.1 Lightweight sandwich insulation wall panel for rural housing 引用方法:JG/T 561 | ||||
| 16 | 16 | 残余拉伸强度/初始拉伸强度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.3.1 Lightweight sandwich insulation wall panel for rural housing 引用方法:JG/T 561 | ||||
| 17 | 17 | 残余层间剪切强度/初始层间剪切强度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.3.1 Lightweight sandwich insulation wall panel for rural housing 引用方法:JG/T 561 | ||||
| 18 | 18 | 屈服强度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.1.3.2、6.1.3.3 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 228.1《金属材料 拉伸试验 第1部分:室温试验方法》 | ||||
| 19 | 19 | 贯通裂缝 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 20 | 20 | 板面污染 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 21 | 21 | 板面裂缝 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 22 | 22 | 大面凹陷 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 23 | 23 | 气泡 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 24 | 24 | 缺棱掉角 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.2 Lightweight sandwich insulation wall panel for rural housing | ||||
| 25 | 25 | 高度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 26 | 26 | 宽度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 27 | 27 | 内叶板厚度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 28 | 28 | 保温板厚度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 29 | 29 | 外叶板厚度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 30 | 30 | 板面平整度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 31 | 31 | 内外板错位 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 32 | 32 | 对角线差 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 33 | 33 | 侧向弯曲 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.3 Lightweight sandwich insulation wall panel for rural housing | ||||
| 34 | 34 | 耐火极限 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.4.1 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 9978.1、GB/T 9978.8 | ||||
| 35 | 35 | 传热系数 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.4.2 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 13475《绝热 稳态传热性质的测定 标定和防护热箱法》 | ||||
| 36 | 36 | 空气声计权隔声量 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.4.3 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 19889.3《声学 建筑和建筑构件隔声测量 第3部分:建筑构件空气声隔声的实验室测量》 | ||||
| 37 | 37 | 抗冲击性能 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.4.4 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 30100《建筑墙板试验方法》 | ||||
| 38 | 38 | 抗弯开裂荷载 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.4.5 Lightweight sandwich insulation wall panel for rural housing | ||||
| 39 | 39 | 抗弯承载力 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 6.4.5 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 15762《蒸压加气混凝土板》 | ||||
| 40 | 40 | 抗冻性 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 7.2.1.1、7.2.1.2 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 11969《蒸压加气混凝土性能试验方法》 | ||||
| 41 | 41 | 抗压强度 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 7.2.1.2 Lightweight sandwich insulation wall panel for rural housing 引用方法:JG/T 350 | ||||
| 42 | 42 | 导热系数 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 7.2.2 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 10294《绝热材料稳态热阻及有关特性的测定 防护热板法》 | ||||
| 43 | 43 | 尺寸稳定性 | 《农村房屋用夹心保温轻质墙板》GB/T46825-2025 7.2.2 Lightweight sandwich insulation wall panel for rural housing 引用方法:GB/T 8811《硬质泡沫塑料 尺寸稳定性试验方法》 | ||||