| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 低多层农村房屋用承重保温一体化墙板及连接配件技术要求 | 1 | 屈服强度 | 100502 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.1.4.3 表2 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | ||
| 2 | 2 | 拉伸强度 | 100502 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.1.4.3 表2 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 3 | 3 | 拉伸弹性模量 | 100502 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.1.4.3 表2 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 4 | 4 | 剪切强度 | 100502 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.1.4.3 表2 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 5 | 5 | 导热系数 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.1.4.3 表2 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 6 | 6 | 钢筋弯折前最大力下的总伸长率 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.1.5.3 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 7 | 7 | 混凝土强度等级 | 100502 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.1.1 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 8 | 8 | 保温材料燃烧性能等级 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.1.3.2 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing 引用方法:GB 8624《建筑材料及制品燃烧性能分级》 | |||
| 9 | 9 | 高度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 10 | 10 | 宽度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 11 | 11 | 厚度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 12 | 12 | 内外板错位 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 13 | 13 | 对角线差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 14 | 14 | 侧向弯曲 | 100502 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 15 | 15 | 扭翘 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 16 | 16 | 表面平整度-内表面 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 17 | 17 | 表面平整度-外表面 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 18 | 18 | 门、窗洞口中心线位置偏差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 19 | 19 | 门、窗洞口宽度、高度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 20 | 20 | 预埋钢板中心线位置偏差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 21 | 21 | 预埋钢板平面高差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 22 | 22 | 预埋螺母中心线位置偏差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 23 | 23 | 预埋螺母外露长度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 24 | 24 | 预埋扣盒、线盒、电盒在墙板平面的水平方向中心位置偏差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 25 | 25 | 预埋扣盒、线盒、电盒与墙板表面混凝土高差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 26 | 26 | 预留孔中心线位置偏移 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 27 | 27 | 预留孔孔尺寸 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 28 | 28 | 预留插筋中心线位置偏移 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 29 | 29 | 预留插筋外露长度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 30 | 30 | 键槽中心线位置偏移 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 31 | 31 | 键槽长度、宽度、深度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 32 | 32 | 预留洞中心线位置偏移 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 33 | 33 | 预留洞洞口尺寸、深度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 34 | 34 | 吊环中心线位置偏移 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 35 | 35 | 吊环与墙板表面混凝土高差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 36 | 36 | 混凝土保护层厚度偏差 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 37 | 37 | 灌浆套筒中心线位置偏移 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 38 | 38 | 安装垂直度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 39 | 39 | 连接钢筋中心线位置 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 40 | 40 | 连接钢筋外露长度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 41 | 41 | 钢筋锚环中心线位置 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 42 | 42 | 钢筋锚环外露长度 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||
| 43 | 43 | 钢丝绳套中心线位置 | 100599 | 《低多层农村房屋用承重保温一体化墙板及连接配件技术要求》GB/T46826-2025 6.3 表4 Technical requirements for integrated load-bearing and insulation wall panels and connecting accessories in low-rise and mid-rise rural housing | |||