| 序号 | 检测对象 | 项目/参数 | 领域代码 | 检测标准(方法)名称及编号(含年号) | 说明 | 备注 | |
|---|---|---|---|---|---|---|---|
| 序号 | 名称 | ||||||
| 1 | 高效空气过滤器性能 | 1 | 上游采样截面风速均匀性偏差 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 5.1.4 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | |||
| 2 | 2 | 上游采样截面气溶胶浓度均匀性偏差 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 5.1.5 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 3 | 3 | 上游气溶胶浓度稳定性波动 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 5.1.6 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 4 | 4 | 上、下游采样相关系数 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 5.1.8 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 5 | 5 | 阻力标件阻力测试偏差 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 5.1.9.3 b) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 6 | 6 | 参考过滤器效率测试值偏差 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 5.1.10.3 a) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 7 | 7 | 偏光故障值 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 5.4.3.3.3 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 8 | 8 | 油雾仪自身散光值 K0 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 5.4.3.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 9 | 9 | NaCl溶液质量浓度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.1 a) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 10 | 10 | 喷雾箱液面距喷孔距离 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.1 a) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 11 | 11 | H2流量 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.1 b) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 12 | 12 | 压缩空气喷雾压力 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.1 d) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 13 | 13 | 喷雾流量 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.1 d) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 14 | 14 | 干燥空气流量 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.1 d) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 15 | 15 | 缓冲箱空气相对湿度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.1 e) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 16 | 16 | 试验体积流量偏差 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 17 | 17 | 过滤前空气流量 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.3.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 18 | 18 | 过滤后空气流量 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.5.3.3.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 19 | 19 | 油雾气溶胶粒子质量平均直径 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 20 | 20 | 油雾发雾剂黏度等级 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.2.3 b) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance 引用方法:GB11120《涡轮机油》 | ||||
| 21 | 21 | 油雾发雾喷雾空气压力 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.2.3 c) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 22 | 22 | 油雾发雾空气加热温度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.2.3 c) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 23 | 23 | 油雾发雾水浴温度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.2.3 c) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 24 | 24 | 油雾发雾油量 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.2.3 c) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 25 | 25 | 进入光电雾室洁净空气流量 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.2.4 a) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 26 | 26 | 进入光电雾室油雾取样流量 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.2.4 b) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 27 | 27 | 油雾仪自身散光值K0 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.3.1 b) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 28 | 28 | 油雾气溶胶浓度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.3.1 c) 1) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 29 | 29 | 油雾法试验空气体积流量偏差 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 6.6.3.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 30 | 30 | 喷雾器工作压力 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.2.2.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 31 | 31 | 干燥后压缩空气含尘浓度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.2.2.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 32 | 32 | 压力表分度值 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.2.2.4 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 33 | 33 | 喷雾器喷头孔径 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.2.3 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 34 | 34 | 喷雾器压缩空气消耗量(3孔) | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 表A.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 35 | 35 | 喷雾器压缩空气消耗量(6孔) | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 表A.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 36 | 36 | 喷雾器压缩空气消耗量(9孔) | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 表A.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 37 | 37 | NaCl发生量(3孔) | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 表A.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 38 | 38 | NaCl发生量(6孔) | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 表A.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 39 | 39 | NaCl发生量(9孔) | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 表A.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 40 | 40 | 混合干燥段直管段长度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.3.1 a) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 41 | 41 | 气溶胶在混合干燥段流动时间 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.3.1 b) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 42 | 42 | 混合干燥段风速 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.3.1 c) Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 43 | 43 | 温度计测量范围 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.3.2.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 44 | 44 | 本底过滤器滤料钠焰法效率 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.4.1.3 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 45 | 45 | 本底过滤器滤料过滤面积 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.4.1.3 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 46 | 46 | 取样管曲率半径 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.4.1.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 47 | 47 | 取样管口流速与风道流速比 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.4.1.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 48 | 48 | 聚光镜焦距 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.4.2.3 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 49 | 49 | Na干涉滤光片波长峰值 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.4.2.3 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 50 | 50 | Na干涉滤光片半波长宽度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.4.2.3 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 51 | 51 | H2源纯度 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.4.2.5 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 52 | 52 | NaCl溶液补液间隔 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.5.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 53 | 53 | NaCl溶液累积使用时间 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.5.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 54 | 54 | NaCl溶液延长使用最长时间 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.5.1 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||
| 55 | 55 | 发雾装置清洗周期 | 《高效空气过滤器性能试验方法 效率和阻力》GB/T6165-2021 A.5.2 Test method of the performance of high efficiency particulate air filter—Efficiency and resistance | ||||